ARCALOY ER312

Arcaloy ER312 is used for welding stainless steels to mild steels and for welding high strength steels difficult to weld with ferritic electrodes.

Ordering Information
SKU256072604
UPC662303049140
Model / Product DescriptionAB ER312 1/16X36X10T/30CT INK
Item Weight10.00
Min Order30
Filler Metal Spec Def 
Size1/16 , 36
Length36 in., 10 in.
Weight10 lbs., Tube lbs.
PackageTube