Arcaloy ER320LR Tigrod is designed for welding Carpenter 20Cb-3® type stainless steels.
| SKU | 256071457 |
|---|---|
| UPC | 662303073282 |
| Model / Product Description | AB ER320LR 1/16X36X10#T/30 INK |
| Item Weight | 10.00 |
| Min Order | 30 |
| Filler Metal Spec Def | |
| Size | 1/16 , 36 |
| Length | 36 in., 10 in. |
| Weight | 10 lbs., Tube lbs. |
| Package | Tube |