ARCALOY ER347

Arcaloy ER347 is a columbium stabilized stainless steel for welding types 347 and 321 stainless, comes in MIG, TIG, and SAW forms.

Ordering Information
SKU258094515
UPC662303027902
Model / Product DescriptionAB ER347 045X33#BAWS
Item Weight33.00
Min Order33
Filler Metal Spec Def 
Size.045
Length33 in.
Weight33 lbs., Spool lbs.
PackageSpool