Arcaloy ER308L is a low carbon grade of 308 designed for MIG or TIG of stainless steels such as AISI 301, 304, 304L steels. SPECIAL ORDER ONLY
| SKU | 257011825 |
|---|---|
| UPC | 662303008352 |
| Model / Product Description | AB ER308L 1/8X60#CL |
| Item Weight | 60.00 |
| Min Order | 60 |
| Filler Metal Spec Def | |
| Size | 1/8 |
| Length | 60 in. |
| Weight | 60 lbs., Coil lbs. |
| Package | Coil |