Dual Shield 710X-M is an all-position flux cored wire for general purpose welding.
| SKU | 245019807 |
|---|---|
| UPC | 662303085063 |
| Model / Product Description | DS 710XM 045X33#AWS |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Length | 33 in. |
| Weight | Spool lbs. |