OK FLUX 282

OK Flux 282 is an active, bonded flux designed for high speed, single pass welding of carbon steel sheet.

Features

OK Flux 282 is an active, bonded flux designed for high speed, single pass welding of carbon steel sheet. Butt, lap, and fillet welds are well washed and free from undercut even at speeds up to 120 IPM (305 cm/min). It is primarily used with DC single and parallel wire systems at currents up to 1300 amps. OK Flux 282 is recommended for making high speed welds in metallic building beams, spiral pipe, storage tanks, and rail cars.

*Single pass application only. Any mechanical property and undiluted weld chemistry listed are for information only.*

OK Flux 282
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS A5.17 F7AZ-EM13K
    • AWS A5.17 F7AZ-EM12K

Properties

Typical Properties
Typical Mechanical Properties  
As Welded  
Spoolarc 81  
Tensile Strength 95 ksi, 655 MPa
Yield Strength 85 ksi, 585 MPa
Elongation in 2" 23 %
CVN 18 ft.-lbs., 24 J
Temperature 0 °F, -18 °C
Spoolarc 29S  
Tensile Strength 100 ksi, 690 MPa
Yield Strength 88 ksi, 605 MPa
Elongation in 2" 22 %
CVN 14 ft.-lbs., 19 J
Temperature 0 °F, -18 °C
Typical Undiluted Weld Metal Analysis  
As Welded  
Spoolarc 81  
C 0.09 %
Mn 1.24 %
Si 0.80 %
P 0.030 %
S 0.020 %
Spoolarc 29S  
C 0.09 %
Mn 1.15 %
Si 1.00 %
P 0.028 %
S 0.014 %

Part No.

Flux 282
Part No. Model / Product Description UPC
8514F09 OK FLUX 282 55#BG 662303078102

SAW

Accessories

Depositions/Paramaters

Extra Info



Basicity Index:0.5
  
Chemical Composition: 
SiO2 + TiO230
Al2 + MnO40
Fluorides<5

Flux Consumption
(lb. Flux / lb. Wire)
VoltageDC+
260.75
300.96
341.36
381.72