Print this page

SUREWELD 10P Plus

Sureweld 10P-Plus is an all-position cellulosic electrode developed for the pipe welding industry. This electrode provides a more consistent burn-off and more forgiving arc burn when compared to Sureweld 10P. It produces X-ray quality joints in all-positions.

Features

Sureweld 10P-Plus is a modified version of the standard 10P electrode and can be differentiated by its gray coating. It has also been developed for the pipe welding industry but has a more consistent burn-off and a more forgiving arc burn. This provides a better bead profile and sidewall fusion with lower spatter. Sureweld 10P-Plus will maintain the proper keyhole in an open root and will produce X-ray quality joints in the flat, horizontal, overhead, vertical-up, and vertical-down procedures. Sureweld 10P-Plus is recommended for welding API grades A25, A, B and X42 pipe and general structural, ship, barge and storage tank fabrication. It may also be used for welding root passes in higher grade pipe in some circumstances.

Sureweld 10P Plus - Web Image Medium
  • Industry
  • Pipeline
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • A.B.S.- AWS A5.1; E6010
    • ASME SFA 5.1
    • CERTIFIED BY C.W.B.- CSA W48
    • AWS A5.1; E6010

Properties

Typical Properties

Part No.

10P Plus
Part No. Model / Product Description UPC
811005511 SW SCASE 10P 1/8 810P 1/8  
811004035 SW 10P PLUS 3/16X14X50#CT 662303050344
811004043 SW 10P PLUS 3/32X12X50#HS 662303050351
811004050 SW 10P PLUS 1/8X14X50#HS 662303050368
811004068 SW 10P PLUS 5/32X14X50#HS 662303050375
811004076 SW 10P PLUS 3/16X14X50#HS 662303050382
811004183 SW 10P PLUS 7/32X18X50#HS 662303050733
811004209 SW 10P PLUS 1/4X18X50#HS 662303050764
811004001 SW 10P PLUS 3/32X12X25#CT 662303050313
811004019 SW 10P PLUS 1/8X14X50#CT 662303050320
811004027 SW 10P PLUS 5/32X14X50#CT 662303050337
811004084 SW 10P PLUS 3/32X12X11#QP 662303050399
811004092 SW 10P PLUS 1/8X14X11#QP 662303050405
811004100 SW 10P PLUS 5/32X14X11#QP 662303050412
811004118 SW 10P PLUS 3/16X14X11#QP 662303050429
811004126 SW 10P PLUS 3/32X12X5#VALP 662303050436
811004134 SW 10P PLUS 1/8X14X5#VALP 662303050443
811004142 SW 10P PLUS 5/32X14X5#VALP 662303050450
811004159 SW 10P PLUS 3/32X12X10#VALP 662303050467
811004167 SW 10P PLUS 1/8X14X10#VALP 662303050474
811004175 SW 10P PLUS 5/32X14X10#VALP 662303050481
811004498 SW 10P PLUS 3/16X14X5#VALP 662303060022

SAW

Accessories

Depositions/Paramaters

Extra Info

Procedure

  • Hold a short arc, but do not allow the coating to touch the molten pool. A slight oscillating motion is recommended in the horizontal and flat positions. Use a short whipping motion on vertical and overhead welds, allowing only enough time out of the crater for the metal to set up. Clean thoroughly between passes. Vertical down and flat position welds should be made at approximately the same amperages.