Sureweld 710P is an E7010-P1 all-position cellulosic electrode developed for pipe welding. This electrode is recommended for welding API pipe grades up to X56. It produces X-ray quality joints in all-positions, with a consistent, deep penetration.

Features

Sureweld 710P is an all-position cellulosic electrode that is especially suited for welding high strength pipe. It produces the consistent, deep penetration required to maintain a proper keyhole when vertical-down welding in open root pipe joints. X-ray quality joints can be produced with Sureweld 710P using flat, horizontal, overhead, vertical-up and vertical-down welding procedures. Sureweld 710P is recommended for welding API grades X46, X52, and X56 pipe. It may also be used for welding root passes in higher grade pipe in some circumstances.

SUREWELD 710P
  • Industry
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5; E7010-P1
    • ASME SFA 5.5
    • (CONFORMS TO E7010-G)
    • CERTIFIED BY C.W.B.- CSA W48

Properties

Typical Properties
As Welded  
Yield Strength 69 ksi, 480 MPa
Tensile Strength 81 ksi, 560 MPa
Elongation in 2" 22 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 29 ft.-lbs., 39 J
Testing Temperature -50ºF (-46ºC)  
As Welded 26 ft.-lbs., 35 J
Typical Undiluted Weld Metal Analysis  
C 0.1 %
Mn 0.3 %
Si 0.2 %
P 0.008 %
S 0.016 %
Ni 0.5 %
Mo 0.24 %

Part No.

710P
Part No. Model / Product Description UPC
811004324 SW SCASE 710P 1/8 5/32 662303064075
811070028 SW 710P 1/8X14X50#HS 662303027964
811070036 SW 710P 5/32X14X50#HS 662303027971
811070044 SW 710P 3/16X14X50#HS 662303027988
811070143 SW 710P 7/32X18X50#HS 662303043872
811070010 SW 710P 3/32X12X50#HS 662303041328
811070150 SW 710P 1/8X14X5#VALP 662303075101
811070168 SW 710P 5/32X14X5#VALP 662303075118

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 75 A 40 - 75 1.5 lbs./hr., 0.7 kg./hr. 72 %
1/8 in, 3.2 mm 100 A 80 - 140 2.1 lbs./hr., 0.9 kg./hr. 76.3 %
130 A 80 - 140 2.3 lbs./hr., 1 kg./hr. 68.8 %
5/32 in, 4.0 mm 140 A 130 - 175 2.8 lbs./hr., 1.3 kg./hr. 73.6 %
170 A 130 - 175 2.9 lbs./hr., 1.3 kg./hr. 64.1 %
3/16 in, 4.8 mm 160 A 150 - 210 3.3 lbs./hr., 1.5 kg./hr. 74.9 %
190 A 150 - 210 3.5 lbs./hr., 1.6 kg./hr. 69.7 %
7/32 in, 5.6 mm 190 A 180 - 275 4.5 lbs./hr., 2 kg./hr. 76.9 %
230 A 180 - 275 5.1 lbs./hr., 2.3 kg./hr. 73.1 %

Extra Info

Procedure

  • Hold a short arc, but do not allow the coating to touch the molten pool. A slight oscillating motion is recommended in the horizontal and flat positions. Use a short whipping motion on vertical and overhead welds, allowing only enough time out of the crater for the metal to set up. Clean thoroughly between passes. Vertical down welds should be made at approximately the same amperages as recommended for the flat position