Print this page

SUREWELD SW-15

Sureweld SW-15 is an all-position electrode that can be used for a wide range of applications for light gauge and heavyplate. High heat and speeds can be used without undercut. The slag is easy to clean and even self-cleaning on heavy plate.

Features

Sureweld SW-15 is a versatile electrode with a wide range of applications for light gauge and heavy plate. High heat and speeds can be used without undercut. Slag is easy to clean and on heavy plates is often self-cleaning.
SW-15 can be used in many applications. Typical applications include metal fixtures, road equipment, farm machinery, building structures, storage tanks and ironwork.

Sureweld SW-15
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.1
    • AWS A5.1; E6013

Properties

Typical Properties
As Welded  
Yield Strength 63 ksi, 435 MPa
Tensile Strength 71 ksi, 490 MPa
Reduction in Area 49 %
Elongation in 2" 24 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 0.3 %
Si 0.2 %
P 0.012 %
S 0.013 %

Part No.

SW-15
Part No. Model / Product Description UPC
811001106 SW 15 3/32X12X25#CT 662303019013
811001114 SW 15 1/8X14X50#CT 662303019020
811001122 SW 15 5/32X14X50#CT 662303019037
811001130 SW 15 3/16X14X50#CT 662303019044
811001148 SW 15 7/32X18X50#CT 662303019051
811001155 SW 15 1/4X18X50#CT 662303019068
811061985 SW 15 3/32X12X50#HS 662303019662
811061134 SW 15 1/8X14X5#VALP 662303053543
811061142 SW 15 3/32X12X5#VALP 662303053581
811061159 SW 15 5/32X14X5#VALP 662303057473
811061167 SW 15 1/8X14X10#VALP 662303057480
811061175 SW 15 3/32X12X10#VALP 662303057497
811061183 SW 15 5/32X14X10#VALP 662303057565
811061902 SW 15 3/32X12X11/44#QP 662303046507
811061910 SW 15 1/8X14X11#QP 662303046514

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
5/64 in, 2.0 mm 50 A 40 - 60 1.4 lbs./hr., 0.6 kg./hr. 73 %
3/32 in, 2.4 mm 85 A 60 - 90 1.6 lbs./hr., 0.7 kg./hr. 73 %
1/8 in, 3.2 mm 125 A 120 - 135 2.1 lbs./hr., 1 kg./hr. 73 %
5/32 in, 4.0 mm 140 A 145 - 190 2.6 lbs./hr., 1.2 kg./hr. 75.6 %
160 A 145 - 190 3 lbs./hr., 1.4 kg./hr. 74.1 %
180 A 145 - 190 3.5 lbs./hr., 1.6 kg./hr. 71.2 %
3/16 in, 4.8 mm 180 A 170 - 230 3.2 lbs./hr., 1.5 kg./hr. 73.9 %
200 A 170 - 230 3.8 lbs./hr., 1.7 kg./hr. 71.1 %
220 A 170 - 230 4.1 lbs./hr., 1.9 kg./hr. 72.9 %
7/32 in, 5.6 mm 250 A 260 - 300 5.3 lbs./hr., 2.4 kg./hr. 71.3 %
270 A 260 - 300 5.7 lbs./hr., 2.6 kg./hr. 73 %
290 A 260 - 300 6.1 lbs./hr., 2.8 kg./hr. 72.7 %
1/4 in, 6.4 mm 290 A 300 - 340 6.2 lbs./hr., 2.8 kg./hr. 75 %
310 A 300 - 340 6.5 lbs./hr., 2.9 kg./hr. 73.5 %
330 A 300 - 340 7.1 lbs./hr., 3.2 kg./hr. 72.1 %