Print this page

SUREWELD SW-15 IP

Sureweld SW-15 IP is an all-position, iron powder coated electrode suitable for welding many types of mild steels in avariety of applications. It’s designed to permit the use of higher welding currents while improving deposition rate. High heats and speeds can be used without undercut, and the slag removal is excellent.

Features

Sureweld SW-15 IP is an iron powder coated electrode permitting the use of higher welding currents while improving the deposition rate. The use of an iron-powder coating also improves deposition efficiency. High speeds and high heats can be used without undercut. Slag removal is excellent. SW-15 IP is widely used for welding mild steels such as ASTM A-36, A-113, A-283, A-284, A-285, A-306, A-515 and A-516. Typical applications include construction equipment, metal fixtures, automotive parts, barges and farm machinery.

SUREWELD SW-15 IP
  • Industry
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.1; E7014
    • ASME SFA 5.1

Properties

Typical Properties
As Welded  
Yield Strength 61 ksi, 420 MPa
Tensile Strength 71 ksi, 490 MPa
Reduction in Area 64 %
Elongation in 2" 28 %
Typical Undiluted Weld Metal Analysis  
C 0.04 %
Mn 0.3 %
Si 0.14 %
P 0.015 %
S 0.019 %

Part No.

SW-15 IP
Part No. Model / Product Description UPC
811001296 SW 15IP 3/32X12X25#CT 662303019075
811001304 SW 15IP 1/8X14X50#CT 662303019082
811001312 SW 15IP 5/32X14X50#CT 662303019099
811001320 SW 15IP 3/16X14X50#CT 662303019105
811001353 SW 15IP 3/32X12X48#HS 662303078836
811001361 SW 15IP 1/8X14X50#HS 662303078843
811001379 SW 15IP 5/32X14X50#HS 662303078850
811041300 SW 15IP 1/8X14X5#VALP 662303057428
811041318 SW 15IP 3/32X12X5#VALP 662303057435
811041326 SW 15IP 5/32X14X5#VALP 662303057442
811041334 SW 15IP 1/8X14X10#VALP 662303057459
811041342 SW 15IP 3/32X12X10#VALP 662303057466
811041359 SW 15IP 5/32X14X10#VALP 662303057558
811041367 SW 15IP 3/32X12X11#QP 662303038052
811041375 SW 15IP 1/8X14X11#QP 662303038069
811041383 SW 15IP 5/32X14X11#QP 662303038076
811041391 SW 15IP 3/16X14X11#QP 662303038083
811041474 SW 15IP 5/32X14X5#CT 662303053987

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 85 A 70 - 100 2 lbs./hr., 0.9 kg./hr. 60 %
1/8 in, 3.2 mm 120 A 100 - 150 2.4 lbs./hr., 1.1 kg./hr. 63.9 %
150 A 100 - 150 3.1 lbs./hr., 1.4 kg./hr. 61.1 %
5/32 in, 4.0 mm 160 A 160 - 200 3 lbs./hr., 1.4 kg./hr. 71.9 %
200 A 160 - 200 3.7 lbs./hr., 1.7 kg./hr. 67 %
3/16 in, 4.8 mm 230 A 190 - 270 4.5 lbs./hr., 2 kg./hr. 70.9 %
270 A 190 - 270 5.5 lbs./hr., 2.5 kg./hr. 73.2 %
7/32 in, 5.6 mm 290 A 230 - 300 5.8 lbs./hr., 2.6 kg./hr. 67.2 %
330 A 230 - 300 7.1 lbs./hr., 3.2 kg./hr. 70.3 %
1/4 in, 6.4 mm 350 A 250 - 350 7.1 lbs./hr., 3.2 kg./hr. 68.7 %
400 A 250 - 350 8.7 lbs./hr., 3.9 kg./hr. 69.9 %

Extra Info

Procedure

Open or drag technique may be used. Use medium to short arc on open arc. When welding vertical-up, tilt the electrode 5º-15º in the direction of travel and use a weaving "U" or "V" arc motion while holding a medium to short arc length. A circular arc motion is perferred for welding overhead. Clean slag thoroughly between passes.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.