Print this page

ATOM ARC 7018-B2L

Atom Arc 7018-B2L is an all-position low hydrogen electrode with an extra low carbon analysis and a 1% Cr - 0.5% Mo weld metal analysis for reduced cracking. These are excellent for power piping, boiler work, castings and forgings.

Features

Atom Arc 7018-B2L is a 1 1/4 Cr - 1/2 Mo electrode with sensitivity extra low carbon content. The low carbon content in the weld metal is beneficial in reducing cracking of weldments. Atom Arc 7018-B2L is carefully engineered to produce a stable arc and good slag release when welding low-alloy steels in the categories of 0.5% Cr - 0.5% Mo, 1% Cr - 0.5% Mo, 1.25% Cr - 0.5% Mo steels. Most grades of these steels are used in power piping, boiler work, castings and forgings

Atom Arc 7018-B2L
  • Industry
  • Pipeline
  • Power Generation
  • Process
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5; E7018-B2LH4R
    • ASME SFA 5.5

Properties

Typical Properties
Stress Relieved 1 hr. @ 1275ºF (691ºC)  
Yield Strength 74 ksi, 510 MPa
Tensile Strength 88 ksi, 607 MPa
Elongation in 2" 29 % %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 0.7 %
Si 0.4 %
P 0.015 %
S 0.016 %
Cr 1.2 %
Mo 0.6 %

Part No.

7018-B2L
Part No. Model / Product Description UPC
255181414 AA 7018-B2L 1/4X18X50#HS 662303018429
255181810 AA 7018-B2L 1/8X14X50#HS 662303018443
255183113 AA 7018-B2L 3/16X14X50#HS 662303018467
255183311 AA 7018-B2L 3/32X14X50#HS 662303018481
255185316 AA 7018-B2L 5/32X14X50#HS 662303018504
255187312 AA 7018-B2L 7/32X18X50#HS 662303018528
255181828 AA 7018-B2L 1/8X14X10#HS 662303018450
255183121 AA 7018-B2L 3/16X14X10#HS 662303018474
255183329 AA 7018-B2L 3/32X14X10#HS 662303018498
255185324 AA 7018-B2L 5/32X14X10#HS 662303018511
255187429 AA 7018-B2L 3/32X12X8#HS/48# 662303031121
255181430 AA 7018-B2L 1/8X14X10#HS XF 662303080921
255181448 AA 7018-B2L 1/8X14X50#HS XF 662303080969
255181455 AA 7018-B2L 3/16X14X10#HS XF 662303080945
255181463 AA 7018-B2L 3/16X14X50#HS XF 662303080983
255181471 AA 7018-B2L 3/32X14X10#HS XF 662303080853
255181489 AA 7018-B2L 3/32X14X50#HS XF 662303080952
255181497 AA 7018-B2L 5/32X14X10#HS XF 662303080938
255181505 AA 7018-B2L 5/32X14X50#HS XF 662303080976
255181513 AA 7018-B2L 7/32X18X50#HS XF 662303080990

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat should be used on hardenable steels to prevent the formation of a hard heat-affected zone. Preheat may also be required in welding heavy sections

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.