Atom Arc 8018-CM is an all-position low hydrogen electrode used for welding steels such as 0.5% Cr - 0.5% Mo, 1% Cr -0.5% Mo, and 1% Cr - 0.5% Mo. Primarily used in power piping and boiler work for the fabrication of plates, pipes, tubes, castings and forging.
Atom Arc 8018-CM electrodes contain 1.25% Cr and 0.50% Mo as alloy addition. They are used for the welding of such steels as 0.5% Cr - 0.5% Mo, 1% Cr - 0.5% Mo, and 1.25% Cr - 0.5% Mo, which are used principally in power piping and boiler work for the fabrication of plates, pipes, tubes, castings, and forgings.

| Stress Relieved 1 hr. @ 1275ºF (691ºC) | |
|---|---|
| Yield Strength | 77 ksi, 535 MPa |
| Tensile Strength | 90 ksi, 620 MPa |
| Reduction in Area | 70 % |
| Elongation in 2" | 26 % |
| Stress Relieved 8 hrs. @ 1275ºF (691ºC) | |
| Yield Strength | 72 ksi, 495 MPa |
| Tensile Strength | 86 ksi, 590 MPa |
| Reduction in Area | 71 % |
| Elongation in 2" | 27 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.07 % |
| Mn | 0.6 % |
| Si | 0.5 % |
| P | 0.016 % |
| S | 0.014 % |
| Cr | 1.23 % |
| Mo | 0.5 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 255051419 | AA 8018-CM 1/4X18X50#HS | 662303017187 |
| 255051815 | AA 8018-CM 1/8X14X50#HS | 662303017194 |
| 255053118 | AA 8018-CM 3/16X14X50#HS | 662303017217 |
| 255053316 | AA 8018-CM 3/32X14X50#HS | 662303017231 |
| 255055311 | AA 8018-CM 5/32X14X50#HS | 662303017255 |
| 255057317 | AA 8018-CM 7/32X18X50#HS | 662303017279 |
| 255057358 | AA 8018-CM 3/32X12X40#HS | 662303017286 |
| 255051823 | AA 8018-CM 1/8X14X10#HS | 662303017200 |
| 255053126 | AA 8018-CM 3/16X14X10#HS | 662303017224 |
| 255053324 | AA 8018-CM 3/32X14X10#HS | 662303017248 |
| 255055329 | AA 8018-CM 5/32X14X10#HS | 662303017262 |
| 255051427 | AA 8018-CM 1/4X18X50#HS XF | 662303081355 |
| 255051435 | AA 8018-CM 1/8X14X10#HS XF | 662303081263 |
| 255051443 | AA 8018-CM 1/8X14X50#HS XF | 662303081317 |
| 255051450 | AA 8018-CM 3/16X14X10#HS XF | 662303081287 |
| 255051468 | AA 8018-CM 3/16X14X50#HS XF | 662303081331 |
| 255051476 | AA 8018-CM 3/32X12X40#HS XF | 662303081294 |
| 255051484 | AA 8018-CM 3/32X14X10#HS XF | 662303081256 |
| 255051492 | AA 8018-CM 3/32X14X50#HS XF | 662303081300 |
| 255051500 | AA 8018-CM 5/32X14X10#HS XF | 662303081270 |
| 255051518 | AA 8018-CM 5/32X14X50#HS XF | 662303081324 |
| 255051526 | AA 8018-CM 7/32X18X50#HS XF | 662303081348 |
| Diameter | Optimal Amperage | Range Amperage | Deposition Rate | Efficiency |
|---|---|---|---|---|
| 3/32 in, 2.4 mm | 90 A | 70 - 100 | 1.7 lbs./hr., 0.8 kg./hr. | 66.3 % |
| 1/8 in, 3.2 mm | 120 A | 90 - 160 | 2.6 lbs./hr., 1.2 kg./hr. | 71.6 % |
| 140 A | 90 - 160 | 2.7 lbs./hr., 1.2 kg./hr. | 70.9 % | |
| 5/32 in, 4.0 mm | 140 A | 130 - 220 | 3.1 lbs./hr., 1.4 kg./hr. | 75 % |
| 170 A | 130 - 220 | 3.8 lbs./hr., 1.7 kg./hr. | 73.5 % | |
| 3/16 in, 4.8 mm | 200 A | 200 - 300 | 4.9 lbs./hr., 2.2 kg./hr. | 76.4 % |
| 250 A | 200 - 300 | 5.4 lbs./hr., 2.4 kg./hr. | 74.6 % | |
| 7/32 in, 5.6 mm | 250 A | 250 - 350 | 6.5 lbs./hr., 2.9 kg./hr. | 75 % |
| 300 A | 250 - 350 | 7.2 lbs./hr., 3.3 kg./hr. | 74 % | |
| 1/4 in, 6.4 mm | 300 A | 300 - 400 | 7.7 lbs./hr., 3.5 kg./hr. | 78 % |
| 350 A | 300 - 400 | 8.7 lbs./hr., 3.9 kg./hr. | 77 % |
Preheat should be used on hardenable steels to prevent the formation of a hard heat-affected zone. Preheat may also be required in welding heavy sections.