Print this page

ATOM ARC 9018-B9

Atom Arc 9018-B9 is designed to weld the modified 9% Cr - 1% Mo steels known by the designations T91, P91 or Grade 91.

Features

Atom Arc 9018-B9 is designed to weld the modified 9% Cr - 1% Mo steels known by the designations T91, P91 or Grade 91. These steels are designed to provide improved creep strength, toughness, fatigue, and oxidation and corrosion resistance at elevated temperatures.

Atom Arc 9018-B9
  • Industry
  • Process
  • Pipeline
  • Petrochemical
  • Power Generation
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5; E9018-B9H4R
    • ASME SFA 5.5

Properties

Typical Properties
Stress Relieved 2 hrs. @ 1375ºF (746ºC)  
Yield Strength 94 ksi, 648 MPa
Tensile Strength 110 ksi, 758 MPa
Elongation in 2" 18 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 72ºF (22ºC) 52 ft.-lbs., 70 J
Typical Undiluted Weld Metal Analysis  
C 0.10 %
Mn 1.0 %
Si 0.2 %
P 0.010 %
S 0.010 %
Cr 9.0 %
Ni 0.2 %
Mo 1.0 %
V 0.2 %
Cu 0.1 %
Nb 0.04 %
N 0.035 %

Part No.

9018-B9
Part No. Model / Product Description UPC
255067803 AA 9018-B9 3/32X14X50#HS XF 662303053017
255067811 AA 9018-B9 1/8X14X50#HS XF 662303053000
255067829 AA 9018-B9 5/32X14X50#HS XF 662303053024
255067837 AA 9018-B9 3/16X14X50#HS XF 662303053031
255067845 AA 9018-B9 3/32X14X10#HS XF 662303053482
255067852 AA 9018-B9 1/8X14X10#HS XF 662303053499
255067860 AA 9018-B9 5/32X14X10#HS XF 662303053505
255067878 AA 9018-B9 3/16X14X10#HS XF 662303053512

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in., 2.4 mm 90 A 70-100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
120 A 90-160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
1/8 in., 3.2 mm 140 A 90-160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
130-220 3.1 lbs./hr., 1.4 kg./hr. 75 %
5/32 in., 4.0 mm 170 A 130-220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
200 A 200-300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
3/16 in., 4.8 mm 250 A 200-300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
250-350 6.5 lbs./hr., 2.9 kg./hr. 75 %
7/32 in., 5.6 mm 300 A 250-350 7.2 lbs./hr., 3.3 kg./hr. 74 %
300-400 7.7 lbs./hr., 3.5 kg./hr. 78 %
1/4 in., 6.4 mm 350 A 300-400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

The recommended preheat temperature for 9CrMo steels is 450-550°F depending on thickness. Post weld heat treatment is generally required.