ATOM ARC 9018

Atom Arc 9018 is an all-position low hydrogen electrode designed for use on high-tensile quenched and tempered steels.

Features

Atom Arc 9018 electrodes are used for attachment welds on T-1, HY-80 and HY-90 steels and other high tensile, quenched and tempered steels.

Atom Arc 9018
  • Industry
  • Shipbuilding
  • Bridge Construction
  • Mobile Machinery
  • General Fabrication
  • Rail Road Car
  • Civil Construction
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.5: E9018M-H4R
    • QPL-22200/1; MIL-9018-M
    • A.B.S.- 3Y
    • L.R.- 3Ym(H15)
    • ASME SFA 5.5

Properties

Typical Properties
As Welded  
Yield Strength 84 ksi, 580 MPa
Tensile Strength 95 ksi, 655 MPa
Reduction in Area 69 %
Elongation in 2" 28 %
Stress Relieved 24 hrs. @ 1100ºF (593ºC)  
Yield Strength 68 ksi, 470 MPa
Tensile Strength 92 ksi, 635 MPa
Reduction in Area 72 %
Elongation in 2" 27 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -60ºF (-51ºC)  
As Welded 60 ft.-lbs., 81 J
Stress Relieved 24 hrs. @ 1100ºF (593ºC) 66 ft.-lbs., 92 J
Typical Undiluted Weld Metal Analysis  
C .043 %
Mn 1.00 %
Si .26 %
P .012 %
S .010 %
Ni 1.60 %
Mo .29 %

Part No.

9018
Part No. Model / Product Description UPC
255061418 AA 9018 1/4X18X50#HS 662303017293
255061806 AA 9018 3/32X14X50#HS 662303017323
255061814 AA 9018 1/8X14X50#HS 662303017330
255061814-03 AA 9018 1/8X14X50#HS 662303060206
255063117 AA 9018 3/16X14X50#HS 662303017354
255065310 AA 9018 5/32X14X50#HS 662303017385
255067316 AA 9018 7/32X18X50#HS 662303025946
255061798 AA 9018 3/32X14X10#HS 662303017316
255061822 AA 9018 1/8X14X10#HS 662303017347
255063125 AA 9018 3/16X14X10#HS 662303017361
255065328 AA 9018 5/32X14X10#HS 662303017392

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat should be used on hardenable steels to prevent the formation of a hard heat-affected zone. Preheat may also be required in welding heavy sections.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.