Print this page

ATOM ARC 7018-AC

Atom Arc 7018-AC is an all-position low hydrogen electrode specifically designed to have optimum arc characteristics when used with AC power sources. It offers easy arc starting, smooth arc and low spatter.

Features

Atom Arc 7018-AC is a product specifically designed to have optimum arc characteristics when used with AC power sources having an open circuit voltage of 75 to 80V. Compared to standard Atom Arc 7018 operating on AC, this electrode will have easier arc starting and restrike, a smoother arc and lower spatter. It is usable on a wide range of steels.

ATOM ARC 7018-AC
  • Industry
  • Civil Construction
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.1; E7018
    • ASME SFA 5.1

Properties

Typical Properties
As Welded  
Yield Strength 77 ksi, 535 MPa
Tensile Strength 86 ksi, 595 MPa
Elongation in 2" 29 %
Reduction in Area 72 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 46 ft.-lbs., 60 J
Typical Undiluted Weld Metal Analysis  
C 0.05 %
Mn 0.9 %
Si 0.3 %
P 0.014 %
S 0.015 %

Part No.

7018-AC
Part No. Model / Product Description UPC
255028508 AA 7018-AC 3/32X14X50#HS 662303016586
255028516 AA 7018-AC 1/8X14X50#HS 662303016593
255028524 AA 7018-AC 5/32X14X50#HS 662303016609
255028573 AA 7018-AC 1/8X14X10#HS 662303016616
255028581 AA 7018-AC 3/32X14X10#HS 662303016623
255028599 AA 7018-AC 5/32X14X10#HS 662303016630
255028623 AA 7018-AC 1/8X14X5#VALP 662303029135
255028631 AA 7018-AC 3/32X14X5#VALP 662303029142
255028649 AA 7018-AC 1/8X14X10#VALP 662303029159
255028656 AA 7018-AC 3/32X14X10#VALP 662303029166
255028664 AA 7018-AC 5/32X14X5#VALP 662303029173
255028672 AA 7018-AC 5/32X14X10#VALP 662303029180
255028680 AA 7018-AC 3/32X14X11#QP 662303029197
255028698 AA 7018-AC 1/8X14X11#QP 662303037819
255028706 AA 7018-AC 5/32X14X11#QP 662303029210
255028771 AA 7018-AC 3/32X12X8#QP 662303041762

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat is generally not required with Atom Arc 7018AC to prevent underbead cracking. Preheat should be used with hardenable steels to prevent the formation of hard heat-affected zones and eliminate tendencies toward quench cracking on cooling. Preheat may also be required in welding heavy sections.