Print this page

ATOM ARC 7018-M

Atom Arc 7018-M is an E7018M all-position low hydrogen electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10.

Features

Atom Arc 7018-M is an all-position low hydrogen electrode specially formulated to meet the more stringent requirements of Military Specification MIL-E-0022200/10 for mechanical properties, coating moisture and diffusible hydrogen content. Atom Arc 7018-M was intended for welding carbon steels, as well as high tensile steels, such as Grade HT of MIL-S-16113 and MIL-S-22698. It is also used for attachment welds to HY-80 and HY-100.

Atom Arc 7018-M
  • Industry
  • Shipbuilding
  • Civil Construction
  • Mobile Machinery
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.1; E7018M
    • A.B.S.- 3,3Y(H5)
    • QPL-22200/10; MIL-7018-M
    • ASME SFA 5.1

Properties

Typical Properties
As Welded  
Yield Strength 69 ksi, 475 MPa
Tensile Strength 80 ksi, 550 MPa
Elongation in 2" 30 %
Reduction in Area 72 %
Stress Relieved 1 hr. @ 1150ºF (621ºC)  
Yield Strength 57 ksi, 395 MPa
Tensile Strength 71 ksi, 490 MPa
Reduction in Area 76 %
Elongation in 2" 36 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 114 ft.-lbs., 155 J
Stress Relieved 1 hr. @ 1150ºF (621ºC) 166 ft.-lbs., 225 J
Typical Undiluted Weld Metal Analysis  
C 0.04 %
Mn 1.0 %
Si 0.3 %
P 0.013 %
S 0.013 %
Mo 0.1 %

Part No.

7018-M
Part No. Model / Product Description UPC
255014003 AA 7018-M 3/32X14X50#HS 662303016234
255014003-03 AA 7018-M 3/32X14X50#HS 662303055431
255014003-25 AA 7018-M 3/32X14X50#HS 662303058982
255014003-34 AA 7018-M 3/32X14X50#HS 662303058012
255014011 AA 7018-M 1/8X14X50#HS 662303016241
255014011-03 AA 7018-M 1/8X14X50#HS 662303055417
255014011-25 AA 7018-M 1/8X14X50#HS 662303056926
255014011-34 AA 7018-M 1/8X14X50#HS 662303058029
255014029 AA 7018-M 5/32X14X50#HS 662303016258
255014029-03 AA 7018-M 5/32X14X50#HS 662303055448
255014037 AA 7018-M 3/16X14X50#HS 662303016265
255014037-03 AA 7018-M 3/16X14X50#HS 662303055424
255014045 AA 7018-M 7/32X18X50#HS 662303016272
255014045-03 AA 7018-M 7/32X18X50#HS 662303057749
255014052 AA 7018-M 1/4X18X50#HS 662303016289
255017501 AA 7018-M 3/32X12X40#HS 662303016579
255118101 GD 7018-M 3/16X14X50#HS 662303054724
255014102 AA 7018-M 3/32X14X10#HS 662303016296
255014102-03 AA 7018-M 3/32X14X10#HS/60# 662303057152
255014110 AA 7018-M 1/8X14X10#HS 662303016302
255014110-05 AA 7018-M 1/8X14X10#HS 662303059224
255014128 AA 7018-M 5/32X14X10#HS 662303016319
255014136 AA 7018-M 3/16X14X10#HS 662303016326
255014151 AA 7018-M 1/4X18X10#HS 662303067946
255118051 GD 7018-M 3/32X12X40#HS 662303029272

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 90 A 70 - 100 1.7 lbs./hr., 0.8 kg./hr. 66.3 %
1/8 in, 3.2 mm 120 A 90 - 160 2.6 lbs./hr., 1.2 kg./hr. 71.6 %
140 A 90 - 160 2.7 lbs./hr., 1.2 kg./hr. 70.9 %
5/32 in, 4.0 mm 140 A 130 - 220 3.1 lbs./hr., 1.4 kg./hr. 75 %
170 A 130 - 220 3.8 lbs./hr., 1.7 kg./hr. 73.5 %
3/16 in, 4.8 mm 200 A 200 - 300 4.9 lbs./hr., 2.2 kg./hr. 76.4 %
250 A 200 - 300 5.4 lbs./hr., 2.4 kg./hr. 74.6 %
7/32 in, 5.6 mm 250 A 250 - 350 6.5 lbs./hr., 2.9 kg./hr. 75 %
300 A 250 - 350 7.2 lbs./hr., 3.3 kg./hr. 74 %
1/4 in, 6.4 mm 300 A 300 - 400 7.7 lbs./hr., 3.5 kg./hr. 78 %
350 A 300 - 400 8.7 lbs./hr., 3.9 kg./hr. 77 %

Extra Info

Preheat is generally not required with Atom Arc 7018-M to prevent underbead cracking. Preheat should be used with hardenable steels to prevent the formation of hard heat-affected zones and eliminate tendencies toward quench cracking on cooling. Preheat may also be required in welding heavy sections.