ARCALOY 308L-15

Arcaloy 308L-15 was developed for welding 304L stainless.

Features

Arcaloy 308L-15 electrodes were developed for the welding of Type 304L stainless steels but can be used for many other stainless steels including Types 301, 302 & 304. They are used extensively for the welding of chemical plant equipment and may be used successfully for the welding of Types 321 and 347 stainless steels provided the service temperature is less than about 700ºF(375ºC). The basic coating of Arcaloy 308L-15 gives the highest resistance to cracking and excellent vertical welding characteristics.

Operates on DC current only.

* This item is subject to Industry Alloy Surcharges

Arcaloy 308L-15
  • Industry
  • Shipbuilding
  • Process
  • Petrochemical
  • General Fabrication
  • Tank and Vessel Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 5
    • ASME II SFA E308-15/E308L-15
    • AWS A5.4; E308-15/E308L-15
    • QPL-22200/2; MIL-308L-15

Properties

Typical Properties
Yield Strength 63 ksi, 430 MPa
Tensile Strength 90 ksi, 520 MPa
Elongation in 2" 45 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.7 %
Si 0.55 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 6 FN

Part No.

308L-15
Part No. Model / Product Description UPC
251021804 AC 308L-15 1/8X14X10#HS 662303013066
251023107 AC 308L-15 3/16X14X10#HS 662303013073
251025300 AC 308L-15 5/32X14X10#HS 662303013097
256120130 AC 308L-15 3/32X12X10#HS 662303049287

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps