Arcaloy 308L-16 was developed for welding 304L stainless.
Arcaloy 308L-16 electrodes were developed for the welding of Type 304L stainless steels but can be used for many other stainless steels including Types 301, 302 & 304. They are used extensively for the welding of chemical plant equipment and may be used successfully for the welding of Types 321 and 347 stainless steels provided the service temperature is less than about 700ºF(375ºC). The basic-rutile thin coating of Arcaloy 308L-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking.
Operates on AC or DC current.
* This item is subject to Industry Alloy Surcharges

| Yield Strength | 66 ksi, 460 MPa |
|---|---|
| Tensile Strength | 90 ksi, 520 MPa |
| Elongation in 2" | 45 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.03 % |
| Mn | 1.7 % |
| Si | 0.5 % |
| Cr | 20 % |
| Ni | 10 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Ferrite | 6 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 251011409 | AC 308L-16 1/4X14X10#HS | 662303012984 |
| 251011805 | AC 308L-16 1/8X14X10#HS | 662303012991 |
| 251013108 | AC 308L-16 3/16X14X10#HS | 662303013004 |
| 251013207 | AC 308L-16 3/32X12X10#HS | 662303074586 |
| 251013306 | AC 308L-16 3/32X9X6#HS SPECIAL ORDER ONLY | 662303013011 |
| 251015301 | AC 308L-16 5/32X14X10#HS | 662303013028 |
| Diameter | Flat | Vertical | Overhead |
|---|---|---|---|
| 1/16 in., 1.6 mm | 20-35 Amps | 15-25 Amps | 20-30 Amps |
| 5/64 in., 2.0 mm | 30-50 Amps | 25-35 Amps | 30-40 Amps |
| 3/32 in., 2.4 mm | 40-70 (Plus 60-85) Amps | 35-50 (40-60) Amps | 40-60 Amps |
| 1/8 in., 3.2 mm | 65-100 (Plus 90-120) Amps | 55-70 (70-80) Amps | 60-85 Amps |
| 5/32 in., 4.0 mm | 100-145 (Plus 140-165) Amps | 85-100 (80-90) Amps | 95-120 Amps |
| 3/16 in., 4.8 mm | 130-190 (Plus 180-210) Amps | 100-115 Amps | 125-150 Amps |
| 1/4 in., 6.4 mm | 205-290 Amps |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.