ARCALOY 308/308H-15

Arcaloy 308/308H-15 is for welding types 304H and 347H stainless when high temperature service is required.

Features

Arcaloy 308/308H-15 electrodes were designed for the welding of Types 304H & 304 for high temperature strength and creep service. They can equally well be used for the welding of stainless steel Types 301, 302 and 305. In some cases where the creep ductility of 347 weld metal is a concern, Arcaloy 308/308H electrodes can be used. The basic coating of Arcaloy 308/308H-15 gives the highest resistance to cracking and excellent verical welding characteristics.

Operates on DC current only.

* This item is subject to Industry Alloy Surcharges

Arcaloy 308/308H-15
  • Industry
  • Petrochemical
  • Process
  • General Fabrication
  • Tank and Vessel Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME II SFA E308-15/308H-15
    • AWS A5.4; E308-15/308H-15
    • QPL-22200/2; MIL-308-15
    • ASME IX F No. 5

Properties

Typical Properties
Tensile Strength 85 ksi, 585 MPa
Elongation in 2" 45 %
Typical Undiluted Weld Metal Analysis  
C 0.05 %
Mn 1.7 %
Si 0.5 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 5 FN

Part No.

308/308H-15
Part No. Model / Product Description UPC
252026497 AC 308/308H-15 3/32X12X10#HS 662303074609
252026513 AC 308/308H-15 1/8X14X10#HS 662303014926
252026521 AC 308/308H-15 5/32X14X10#HS 662303014933

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps