Print this page

ARCALOY 308/308H-16

Arcaloy 308/308H-16 was developed for welding types 304H and 347H stainless when high temperature service is required.

Features

Arcaloy 308/308H-16 electrodes were designed for the welding Types 304H & 304 where temperature in excess of 700°F(375°C) requires additional creep strength. They can equally well be used for the welding of stainless steel Types 301, 302 and 305. In some cases where the creep ductility of 347 weld metal is a concern, Arcaloy 308/308H electrodes can be used. The basic-rutile thin coating of Arcaloy 308/308H-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking.

Operates on AC or DC current.

* This item is subject to Industry Alloy Surcharges

Arcaloy 308/308H-16
  • Industry
  • Process Piping
  • Food and Beverage
  • Tank and Vessel Fabrication
  • Petrochemical
  • Power Generation
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME II SFA E308-16/E308H-16
    • AWS A5.4; E308-16/E308H-16
    • Certified by CWB to CSA W48
    • ASME IX F No. 5
    • MIL-E-22200/2 MIL-308-16

Properties

Typical Properties
Yield Stress 66 ksi, 410 MPa
Tensile Strength 89 ksi, 610 MPa
Elongation in 2" 44 %
Typical Undiluted Weld Metal Analysis  
C 0.055 %
Mn 1.7 %
Si 0.45 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.1 %
Ferrite 6 FN

Part No.

308/308H-16
Part No. Model / Product Description UPC
252026539 AC 308/308H-16 3/32X9X6#HS SPECIAL ORDER ONLY 662303014940
252026547 AC 308/308H-16 1/8X14X10#HS 662303014957
252026554 AC 308/308H-16 5/32X14X10#HS 662303014964
252026562 AC 308/308H-16 3/32X12X10#HS 662303074593
252026612 AC 308/308H-16 3/16X14X10#HS 662303014988
252026620 AC 308/308H-16 1/4X14X10#HS 662303014995

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.