ARCALOY 309MoL-15

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. Ideal for cladding prior to joining stainless steel to low alloy steels. Best used out-of-position on DC current.

Features

Arcaloy 309MoL-15 is designed for applications requiring molybdenum with a standard 309L analysis. It is used primarily for welding Types 316L and 316 clad steels, or for the first layer of a molybdenum - bearing stainless steel cladding on mild or low alloy steels austenitic stainless steels - to carbon and low alloy steels, provided the service temperature is less than about 600ºF (316ºC). In the dissimilar joint, Arcaloy 309MoL can tolerate more dilution by carbon and low alloy steels than Arcaloy 309L-15. Post weld heat treatment should be given due consideration.

* This item is subject to Industry Alloy Surcharges

309MoL-15
  • Industry
  • Process
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E309MoL-15/E309Mo-15
    • ASME IX F No. 5
    • ASME II SFA E309Mol-15/E309Mo-15

Properties

Typical Properties
Yield Stress 75 ksi, 510 MPa
Tensile Strength 95 ksi, 650 MPa
Elongation in 2" 39 %
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 1.7 %
Si 0.6 %
Cr 22.7 %
Ni 13.4 %
Mo 2.3 %
Cu 0.1 %
Ferrite 16 FN

Part No.

309MoL-15
Part No. Model / Product Description UPC
251091807 AC 309LMO-15 1/8X14X10#HS 662303013585
251095303 AC 309LMO-15 5/32X14X10#HS 662303013608
251095584 AC 309LMO-15 3/32X12X10#HS  

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Volts 15-25 Volts 20-30 Volts
5/64 in., 2.0 mm 30-50 Volts 25-35 Volts 30-40 Volts
3/32 in., 2.4 mm 40-70 (Plus 60-85) Volts 35-50 (40-60) Volts 40-60 Volts
1/8 in., 3.2 mm 65-100 (Plus 90-120) Volts 55-70 (70-80) Volts 60-85 Volts
5/32 in., 4.0 mm 100-145 (Plus 140-165) Volts 85-100 (80-90) Volts 95-120 Volts
3/16 in., 4.8 mm 130-190 (Plus 180-210) Volts 100-115 Volts 125-150 Volts
1/4 in., 6.4 mm 205-290 Volts

Extra Info

Arcaloy 309MoL electrodes are used for welding carbon and low alloy steels to stainless steels provided the service temperature does not exceed about 700ºF (370ºC). These electrodes have a higher potential ferrite content than the Arc 309L electrodes and can tolerate higher levels of dilution. If the joint is thick, the low alloy side should be buttered with these electrodes (PWHT only if required) and the joint made with Arcaloy 316LF5 electrodes. Arcaloy 309MoL electrodes are used for the first layer of 316L or 317L cladding. The basic - rutile thin coating of Arcaloy 309MoL-15 gives an excellent combination of welding performance in all positions and a high resistance to cracking. It is therefore a good choice for a multitude of welding applications including tight joints.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.