Arcaloy 310-16

Arcaloy 310-16 electrodes were developed for the welding of type 310 stainless steel. Usable on AC or DC current.

Features

Arcaloy 310 electrodes were developed for the welding of type 310 stainless steel. Arcaloy 310 weld deposit exhibits the same chemical analysis and oxidation resistance as the base plate metal. It is considered standard practice to weld types 410, 430, and 502 with Arcaloy 310 or 309 where field welding is done and where it is not possible to preheat or anneal after welding.

* This item is subject to Industry Alloy Surcharges

Classifications

  • Classifications/Approvals

    • QPL 22200/2; MIL 310-16
    • ASME II SFA E310-16
    • ASME IX F No. 5
    • AWS A5.4; E310-16

Properties

Typical Properties
Yield Stress 65 ksi, 450 MPa
Tensile Strength 90 ksi, 610 MPa
Elongation in 2" 38 %
Typical Undiluted Weld Metal Analysis  
C 0.1 %
Mn 1.8 %
Si 0.5 %
Cr 26 %
Ni 21 %
Mo 0.1 %
Cu 0.1 %

Part No.

310-16
Part No. Model / Product Description UPC
251101408 AC 310-16 1/4X14X10#HS 662303013677
251101804 AC 310-16 1/8X14X10#HS 662303013684
251103107 AC 310-16 3/16X14X10#HS 662303013691
251103313 AC 310-16 3/32X12X10#HS 662303074654
251105300 AC 310-16 5/32X14X10#HS 662303013714

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info

Arcaloy 310 electrodes are used for welding of Type 310 stainless steels. They should not be used for the high carbon grades of similar composition such as the ACI Grade HK-40 owing to the likelihood of weld metal cracking. Arcaloy 310 weld metal is ferrite free and therefore non-magnetic but the possibility of micro-fissuring cannot be ruled out. The use of Arcaloy 310-16 in this respect may be preferred. The basic-rutile thin coating of Arcaloy 310-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking. It is therefore a good choice for a multitude of welding applications including tight joints.