Arcaloy 312-16

Arcaloy 312-16 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys. Usable on AC or DC current.

Features

Arcaloy 312 electrodes were originally designed for welding of high tensile alloys to high temperature heat-resisting alloys on turbo-jet engines of that time. However, based upon performance, these electrodes have found wide acceptance for the welding of high carbon steels high yield steels and abrasion resisting steels and those steels to stainless steels. The high strength of the "all weld metal" deposit is usually reduced by dilution with a dissimilar base metal.

* This item is subject to Industry Alloy Surcharges

312-16
  • Industry
  • General Fabrication
  • Pulp and Paper
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.4; E312-16
    • MIL-E-22200/2 MIL-312-16
    • ASME II SFA E312-16
    • ASME IX F No. 5

Properties

Typical Properties
Yield Stress 85 ksi, 600 MPa
Tensile Strength 115 ksi, 800 MPa
Elongation in 2" 25 %
Typical Undiluted Weld Metal Analysis  
C 0.11 %
Mn 1.8 %
Si 0.5 %
Cr 29 %
Ni 9.7 %
Mo 0.1 %
Cu 0.1 %
Ferrite 50 FN

Part No.

312-16
Part No. Model / Product Description UPC
251161808 AC 312-16 1/8X14X10#HS 662303013936
251163101 AC 312-16 3/16X14X10#HS 662303013943
251163309 AC 312-16 3/32X9X6#HS SPECIAL ORDER ONLY 662303013950
251163317 AC 312-16 3/32X12X10#HS 662303074661
251165304 AC 312-16 5/32X14X10#HS 662303013967

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info

Arcaloy 312-16 electrodes are used for welding carbon and low alloy steels to themselves, similar steels or stainless steels provided the service temperature does not exceed about 700ºF (370ºC). They can tolerate higher carbon levels in the base metal and higher levels of dilution than other stainless steel electrodes. In many cases, no preheat is necessary provided the carbon level of the steel is less than 0.3%. For higher levels of carbon, a preheat to 300ºF (150ºC) is often sufficient to prevent hydrogen cracking. If these welds were made with a carbon or low alloy steel electrode, higher temperature preheats would be necessary. Arcaloy 312-16 electrodes, especially Arcaloy 312-16, are the electrodes of choice to attempt to weld various grades of free-machining steels that do not contain lead. In the welding of free-machining steels special low stress techniques should be used and even so, success cannot be assured. Care must be taken however when applying these electrodes. Insufficient dilution appropriate to the steel involved, high preheat temperatures and heat input over a period of time or PWHT can embrittle the weld metal that can lead to cracking. In a similar manner, the HAZ of high carbon steels can be free of cracking due to the use of these electrodes but can be hard and brittle with a potential for cracking. The high chromium content gives good oxidation resistance at high temperatures provided an embrittled structure can be tolerated. The high chromium content coupled with the duplex structure gives one of the best compositions for corrosion resistance in pulp digesters and allied equipment. For that reason, 312 filler metals are used for cladding in these applications. The basic coating of Arcaloy 312-16 gives the highest resistance to cracking and excellent vertical welding characteristics. It is therefore the choice for field welding.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.