ARCALOY 316/316H-15

Arcaloy 316/316H-15 can be used in applications where 316 stainless needs improved due to higher service temperature. Best used out-of-position on DC current.

Features

Arcaloy 316/316H-15 can be used for welding Type 316 and should be used in applications where 316 or 316H stainless needs improved high temperature. In some cases, E16-8-2 electrodes should be used.

* This item is subject to Industry Alloy Surcharges

316/316H-15
  • Industry
  • Petrochemical
  • General Fabrication
  • Process
  • Steel Industry
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME II SFA E316-15/E316H-15
    • QPL-22200/2; MIL-316-15
    • ASME IX F No. 5
    • AWS A5.4; E316-15/E316H-15

Properties

Typical Properties
Yield Strength 66 ksi, 490 MPa
Tensile Strength 86 ksi, 590 MPa
Elongation in 2" 40 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 1.6 %
Si 0.4 %
Cr 19 %
Ni 11.5 %
Mo 2.3 %
Cu 0.2 %
Ferrite 6 FN

Part No.

316/316H-15
Part No. Model / Product Description UPC
251186508 AC 316/316H-15 1/8X14X10#HS 662303043117
251186557 AC 316/316H-15 3/32X12X10#HS 662303074708

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 125-150 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info

Arcaloy 316/316H-15 electrodes are used for welding Type 316 stainless steel and should be used where high temperature occur in service. The basic coating of Arcaloy 3169/316H-15 gives the highest resistance to cracking and excellent vertical welding characteristics. It is therefore the choice for field welding.