Print this page

CRYOARC 316L-15

Cryoarc 316L-15 is a covered electrode designed for low temperature cryogenic applications. Pre-test lot controlled formulation to maximize mechanical properties. Best used out-of-position on DC current.

Features

Cryoarc 316L-15 electrodes are designed to be used in cryogenic applications where impact toughness is required. Cryoarc 316L-15 electrodes can also be used where low magnetic permeability is required.

* This item is subject to Industry Alloy Surcharges

316L-15
  • Industry
  • Cryogenic
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 5
    • ASME II SFA 5.4 E316L-15
    • A.B.S. AWS A5.4 E316L-15

Properties

Typical Properties
Yield Strength 53 ksi, 370 MPa
Tensile Strength 75 ksi, 520 MPa
Lateral Expansion 30 mils, 0.76 mm
Magnetic Permeability 1.1 µ
Elongation in 2" 40 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -320ºF (-196ºC) 33 ft.-lbs., 45 J
Typical Undiluted Weld Metal Analysis  
C 0.03 %
Mn 2 %
Si 0.5 %
Cr 18 %
Ni 13.5 %
Mo 2.2 %
Ferrite 0.5 FN (2FN max) FN

Part No.

316L-15
Part No. Model / Product Description UPC
257171801 CRYOARC 316L-15 1/8X14X10#HS 662303015718
257173104 CRYOARC 316L-15 3/16X14X10#HS 662303015725
257173302 CRYOARC 316L-15 3/32X9X6#HS 662303015732
257175307 CRYOARC 316L-15 5/32X14X10#HS 662303015756

SAW

Accessories

Depositions/Paramaters

Welding Parameters
Diameter Flat Vertical Overhead
1/16 in., 1.6 mm 20-35 Amps 15-25 Amps 20-30 Amps
5/64 in., 2.0 mm 30-50 Amps 25-35 Amps 30-40 Amps
3/32 in., 2.4 mm 40-70 (Plus 60-85) Amps 35-50 (40-60) Amps 40-60 Amps
1/8 in., 3.2 mm 65-100 (Plus 90-120) Amps 55-70 (70-80) Amps 60-85 Amps
5/32 in., 4.0 mm 100-145 (Plus 140-165) Amps 85-100 (80-90) Amps 95-120 Amps
3/16 in., 4.8 mm 130-190 (Plus 180-210) Amps 100-115 Amps 95-120 Amps
1/4 in., 6.4 mm 205-290 Amps

Extra Info

Cryoarc 316L-15 is designed to be used in cryogenic and LNG applications where greater impact toughness is required. It can also be used where low magnetic permeability is required. The basic coating gives the highest resistance to cracking and excellent vertical welding characteristics. It is therefore the choice for field welding.