ARCALOY 8N12

Arcaloy 8N12 electrodes are intended for the welding of high nickel alloys to other nickel alloys, stainless and low alloy steels.

Features

Arcaloy 8N12 is used to join UNS 06600 alloys e.g. Inconel* 600 and some other nickel alloys. It is used for many applications welding dissimilar joints between nickel alloys, stainless and low alloy steels. It should be used to join stainless steels to CrMo steels for service in the 700-1100ºF(375-600ºC) range.

* This item is subject to Industry Alloy Surcharges

Arcaloy 8N12
  • Industry
  • Process
  • Petrochemical
  • Power Generation
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 43
    • ASME II SFA 5.11 ENiCrFe-3

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength 54 ksi, 370 MPa
Yield Strength 85 ksi, 580 MPa
Elongation in 2" 36 %

Part No.

8N12
Part No. Model / Product Description UPC
258075977 AC 8N12 3/32X12X8#HS 662303015879
258075985 AC 8N12 1/8X14X10#HS 662303015886
258075993 AC 8N12 5/32X14X10#HS 662303015893