ARCALOY 276

Arcaloy 276 is a NiCrMo-4 alloy designed for joining, cladding or surfacing nickel based alloys and stainless steel.

Features

Arcaloy 276 is designed for joining Alloy C-276 and other NiCrMo alloys. It is also sometimes used to join high Mo austenitic stainless steels, joining Ni based alloys to stainless or low alloy steels as well as for the cladding of low alloy steels.

* This item is subject to Industry Alloy Surcharges

ARCALOY 276
  • Industry
  • Process
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 44
    • ASME II SFA 5.11 ENiCrMo-4

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength 106 ksi, 730 MPa
Yield Strength 79 ksi, 545 MPa
Elongation in 2" 39 %

Part No.

276
Part No. Model / Product Description UPC
256071762 AC 276 1/8X14X10#HS 662303049911
256071770 AC 276 5/32X14X10#HS 662303049928
256071788 AC 276 3/16X14X10#HS 662303049935