OK 92.55

OK 92.55 is designed to weld 9% nickel steels giving an optimum strength and toughness combination down to 320°F (-196°C).

Features

OK 92.55 can be used to weld low alloyed steels where impact toughness is paramount. OK 92.55 was developed for use on LNG storage tanks. Best used on DCEP(DC electrode positive).

* This item is subject to Industry Alloy Surcharges

OK 92.55
  • Industry
  • Process
  • Petrochemical
  • Power Generation
  • Pipeline
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.11; ENiCrMo-6

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength 102 ksi, 710 MPa
Yield Strength 65 ksi, 450 MPa
Elongation in 2" 40 %

Part No.

92.55
Part No. Model / Product Description UPC
92552530K0 ES OK92.55 2.5X300X7.2KG VP 662303080648
92553230G0 ES OK92.55 3.2X350X12KG VP 662303080655
92554030G0 ES OK92.55 4.0X350X13.2KG VP 662303080662
92555030G0 ES OK92.55 5.0X350X12.6KG VP 662303080679