Arcaloy 9N10 is intended to weld Monel* 400 to low alloy and stainless steels.
Acaloy 9N10 is used for joining nickel-copper alloy N04400 (Monel* 400) to itself and to carbon, low alloy and some stainless steels.
*Monel is a registered trademark of the Special Metals Corporation
* This item is subject to Industry Alloy Surcharges

| Typical Mechanical Properties | |
|---|---|
| Tensile Strength | 75 ksi, 515 MPa |
| Yield Strength | 52 ksi, 360 MPa |
| Elongation in 2" | 40 % |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.