Print this page

NICKEL-ARC 55

Nickel-Arc 55 is designed for welding nodular cast iron to steel. This electrode's deposit is sound, crack-free and produces good color matching on gray malleable or nodular cast iron.

Features

This electrode is made with a composite 55% nickel and 45% iron core, designed for welding cast iron (ie: nodular) to steel. Proper welding procedures should be followed.

* This item is subject to Industry Alloy Surcharges

NickelArc 55
  • Industry
  • General Cast Iron Repair and Fabrication
  • Rail Road Car
  • Mobile Machinery
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • AWS A5.15; ENiFe-CI-A
    • ASME SFA 5.15

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength 58 ksi, 400 MPa
Weld Hardness 165-218 BHN
Typical Undiluted Weld Metal Analysis  
C 1.3 %
Mn 0.6 %
Si 0.6 %
Ni 48 %
Al 1.4 %

Part No.

55
Part No. Model / Product Description UPC
253041826 NA 55 1/8X14X10#HS 662303015107
253043129 NA 55 3/16X14X10#HS 662303015121
253043301 NA 55 3/32X9X6#HS 662303015138
253045322 NA 55 5/32X14X10#HS 662303015152

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.