Print this page

ESAB ER4043

ESAB 4043 is an aluminum solid wire used for general purpose welding and brazing.

Features

ESAB 4043 is one of the oldest and most widely used welding and brazing alloys. It can be classified as a general purpose type filler alloy. The silicon additions result in improved fluidity to make the alloy a preffered choice by welders. The salloy is less sensitive to weld cracking and produces brighter, almost smut free welds.

ESAB ER4043
  • Industry
  • General Fabrication
  • Automotive
  • Mobile Machinery
  • Shipbuilding
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS A5.10; ER4043

Properties

Typical Properties
Typical Mechanical Properties  
As Welded  
Base Alloy 2014-T6  
Tensile Strength 34 ksi, 235 MPa
Yield Strength 28 ksi, 195 MPa
Elongation in 2" 4 %
Base Alloy 6061-T4  
Tensile Strength 27 ksi, 185 MPa
Yield Strength 18 ksi, 125 MPa
Elongation in 2" 8 %
Base Alloy 6061-T6  
Tensile Strength 27 ksi, 185 MPa
Yield Strength 18 ksi, 125 MPa
Elongation in 2" 8 %
Base Alloy 6063-T4  
Tensile Strength 20 ksi, 140 MPa
Yield Strength 10 ksi, 70 MPa
Elongation in 2" 12 %
Other Typical Mechanical Properties  
Melting Range 1065 to 1170 °F, 574 to 632 °C
Density .097 lbs/cu. in.
Anodize Color Gray
Wire Analysis (Single Values Minimum)  
Mn 0.05 %
Si 4.5-6.0 %
Ti 0.20 %
Cu 0.30 %
Mg 0.05 %
Zn 0.10 %
Be 0.0008 %
Fe 0.8 %

Part No.

ER4043HQ
Part No. Model / Product Description UPC
5202F04 4043HQ 030X14#SP 662303055868
5202F05 4043HQ 035X16#SP 662393012611
5202F07 4043HQ 3/64X16#SP 662393012437
5202F08 4043HQ 1/16X16#SP 662303068684
5202F10 4043HQ 3/32X16#SP 662303068691
5202F84 4043HQ 030X1#SP/18#CT 662303058166
5202F85 4043HQ 035X1#SP/18#CT 662303058173
5202F87 4043HQ 3/64X1#SP/18#CT 662393012444
5202F88 4043HQ 1/16X1#SP/18#CT 662303068707
5203F07 4043HQ 3/64X167#RL/501#PLT 662303068721
5203F08 4043HQ 1/16X167#RL/501#PLT 662303068738
5206F87 4043HQ 3/64X20#SP 662303055875
5206F88 4043HQ 1/16X20#SP 662303068745
5021F07 4043HQ 3/64X36X10#TX60#CT 662303059255
5021F08 4043HQ 1/16X36X10T/40CT 662303058135
5021F10 4043HQ 3/32X36X10T/40CT 662303055783
5021F12 4043HQ 1/8X36X10T/40CT 662303055844
5021F14 4043HQ 5/32X36X10T/40CT 662303058197
5021F15 4043HQ 3/16X36X10T/40CT 662303066239
180408215A 4043 030X1#PSP/18#CT 662303080280
180408245A 4043 030X14#PSP 662303080310
180409215A 4043 035X1#PSP/18#CT 662303080297
180409243A 4043 035X16#PSP 662303080327
180410243A 4043 040X16#PSP 662303080877
180410944A 4043 040X311#OMP 662303080884
180412215A 4043 3/64X1#PSP/18#CT 662303080303
180412242A 4043 3/64X20#PSP 662303080358
180412243A 4043 3/64X16#PSP 662303080334
180416242A 4043 1/16X20#PSP 662303080365
180416243A 4043 1/16X16#PSP 662303080341
180416944A 4043 1/16X311#OMP  
180416R15A 4043 1/16X39X11#CT/33#CT 662303080464
180424R15A 4043 3/32X39X11#CT/33#CT 662303080471
180432R15A 4043 1/8X39X11#CT/33#CT 662303080488
180440R15A 4043 5/32X39X11#CT/33#CT 662303080495
180450R15A 4043 3/16X39X11#CT/33#CT 662303080501

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.