Print this page

ESAB ER5356

ESAB 5356 is an aluminum solid wire used for moderate high strength welding.

Features

ESAB 5356 is a non-heat treable solid aluminum wire for moderate high strength applications. Principle alloy elements include Mangnesium, Manganese, Chromium and Titanium.

ESAB ER5356
  • Industry
  • Mobile Machinery
  • Shipbuilding
  • Automotive
  • General Fabrication
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS A5.10; ER5356

Properties

Typical Properties
Typical Mechanical Properties  
As Welded  
Base Alloy 6061-T6  
Tensile Strength 30 ksi, 210 MPa
Yield Strength 19 ksi, 130 MPa
Elongation in 2" 11 %
Base Alloy 6063-T6  
Tensile Strength 20 ksi, 140 MPa
Yield Strength 12 ksi, 85 MPa
Elongation in 2" 12 %
Base Alloy 7005-T6  
Tensile Strength 46 ksi, 315 MPa
Yield Strength 30 ksi, 205 MPa
Elongation in 2" 10 %
Base Alloy 7039-T-64  
Tensile Strength 44 ksi, 305 MPa
Yield Strength 25 ksi, 170 MPa
Elongation in 2" 13 %
Other Typical Mechanical Properties  
Melting Range 1060 to 1175 °F, 571 to 635 °C
Density .096 lbs/cu. in.
Anodize Color White
Wire Analysis (Single Values Minimum)  
Mn 0.05-0.20 %
Si 0.25 %
Cr 0.05-0.20 %
Ti 0.06-0.20 %
Cu 0.10 %
Mg 4.5-5.5 %
Zn 0.10 %
Be 0.0008 %
Fe 0.40 %

Part No.

ER5356HQ
Part No. Model / Product Description UPC
5182F04 5356HQ 030X14#SP 662303058210
5182F05 5356HQ 035X16#SP 662393012420
5182F07 5356HQ 3/64X16#SP 662303513122
5182F08 5356HQ 1/16X16#SP 662393012475
5182F10 5356HQ 3/32X16#SP 662303068615
5182F84 5356HQ 030X1#SP/18#CT 662303058180
5182F85 5356HQ 035X1#SP/18#CT 662303058159
5182F87 5356HQ 3/64X1#SP/18#CT 662393012468
5182F88 5356HQ 1/16X1#SP/18#CT 662303068622
5186F87 5356HQ 3/64X20#SP 662303078072
5186F88 5356HQ 1/16X20#SP 662303068660
5051F08 5356HQ 1/16X36X10T/40CT 662303058142
5051F10 5356HQ 3/32X36X10T/40CT 662303055790
5051F12 5356HQ 1/8X36X10T/40CT 662303055813
5051F14 5356HQ 5/32X36X10T/40CT 662303066277
5051F15 5356HQ 3/16X36X10T/40CT 662303058203
181508215A 5356 030X1#PSP/18#CT 662303080372
181508245A 5356 030X14#PSP 662303080402
181509215A 5356 035X1#PSP/18#CT 662303080389
181509243A 5356 035X16#PSP 662303080419
181512215A 5356 3/64X1#PSP/18#CT 662303080396
181512242A 5356 3/64X20#PSP 662303080440
181512243A 5356 3/64X16#PSP 662303080426
181512944A 5356 3/64X311#OMP 662303080792
181516242A 5356 1/16X20#PSP 662303080457
181516243A 5356 1/16X16#PSP 662303080433
181516R15A 5356 1/16X39X11#CT/33#CT 662303080518
181524R15A 5356 3/32X39X11#CT/33#CT 662303080525
181532R15A 5356 1/8X39X11#CT/33#CT 662303080532
181540R15A 5356 5/32X39X11#CT/33#CT 662303080549
181550R15A 5356 3/16X39X11#CT/33#CT 662303080556
5051F13 5356HQ 3/64X36X10#T/60#CT 662303080068

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.