OK Autrod 308L is a low carbon MIG wire and has good general corrosion resistance.
OK Autrod 308L is a continuous, solid, corrosion-resistant, chromium-nickel wire. The alloy has a low carbon content which makes this alloy particularly recommended were there is a risk of intergranular corrosion. For joining of stainless steels of 18% Cr - 8% Ni type and Nb-stabilized steels of the same type if the service temperature will not exceed 662°F (350°C).
* This item is subject to Industry Alloy Surcharges

| C | <0.03 % |
|---|---|
| Mn | 1.8 % |
| Si | 0.5 % |
| Cr | 20.3 % |
| Ni | 10.0 % |
| Mo | <0.3 % |
| Cu | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 161024311A | ES OK ER308L 3/32X55#CL | 000000000000 |
| 161032311A | ES OK ER308L 1/8X55#CL | 000000000000 |
| 161040311A | ES OK ER308L 5/32X55#CL | 000000000000 |
| 161016311A | ES OK ER308L 1/16X55#CL | 662303077556 |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.2-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in, 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in, 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in, 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.75 kg./hr. |
| .035 in, 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr. |
| .045 in, 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr. |