Arcaloy ER308LSi is a silicon enhanced MIG wire which significantly increases wetting action, resulting in a smooth weld to improve weldability and performance on 304 steels.
OK Arcaloy ER308LSi is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18 Cr- 8% Ni type. The alloy has a low carbon content, making it particularly recommended where there is a risk of intergranular corrosion.
* This item is subject to Industry Alloy Surcharges

| GMAW using 98% Argon / 2% Oxygen | |
|---|---|
| Yield Stress | 55 ksi, 380 MPa |
| Tensile Strength | 85 ksi, 690 MPa |
| Elongation in 2" | 40 % |
| Typical Chemical Analysis | |
| C | 0.015 % |
| Mn | 1.7 % |
| Si | 0.8 % |
| S | 0.01 % |
| Cr | 20 % |
| Ni | 10 % |
| Mo | 0.1 % |
| Cu | 0.2 % |
| Ferrite | 10 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 258123140 | AB ER308LSI 035X500#OMP | 662303667733 |
| 258123538 | AB ER308LSI 045X500#OMP | 662303667634 |
| 258121110 | AB ER308LSI 1/16X33#PSP | 662303027520 |
| 258123025 | AB ER308LSI 030X10#PSP/60CT | 662303027483 |
| 258123116 | AB ER308LSI 030X33#PSP | 662303027506 |
| 258123157 | AB ER308LSI 035X250#OMP 2/PLT | 662303523589 |
| 258123306 | AB ER308LSI 030X2#4 SP/40#CT | 662393013304 |
| 258123512 | AB ER308LSI 035X33#BAWS | 662303027513 |
| 258123975 | AB ER308LSI 045X250#OMP 2/PLT | 662303667726 |
| 258124510 | AB ER308LSI 045X33#BAWS | 662303026387 |
| 258125525 | AB ER308LSI 035X10#PSP/60CT | 662303027490 |
| 257011163 | AB ER308LSI 023X10#PSP |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr |
| .035 in., 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr |
| .045 in., 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg/hr |
| .035 in., 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg/hr |
| .045 in., 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg/hr |
| .062 in., 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg/hr |