OK Autrod 309L is a continuous, solid, corrosion-resistant, chromium-nickel wire for welding of similar steels, wrought and cast steels of 23% Cr - 12% Ni types.
OK Autrod 309L is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld. OK Autrod 309L has good general corrosion resistance. When used for joining dissimilar materials the corrosion resistance is of secondary importance.
* This item is subject to Industry Alloy Surcharges

| Yield Strength | 64 ksi, 440 MPa |
|---|---|
| Tensile Strength | 87 ksi, 600 MPa |
| Elongation in 2" | 41 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -76°F (-60°C) | 96 ft.-lbs, 130 J |
| Testing Temperature -166°F (-110°C) | 66 ft.-lbs, 90 J |
| Testing Temperature 68ºF (20ºC) | 118 ft.-lbs., 160 J |
| Typical wire analysis | |
| C | 0.03 % |
| Mn | 1.5 % |
| Si | 0.4 % |
| P | 0.010 % |
| S | 0.005 % |
| Cr | 23.5 % |
| Ni | 12.5 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 165324311A | ES OK ER309L 3/32X55#CL | 000000000000 |
| 165332311A | ES OK ER309L 1/8X55#CL | 000000000000 |
| 165340311A | ES OK ER309L 5/32X55#CL | 000000000000 |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in, 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in, 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in, 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in, 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr. |
| .035 in, 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr. |
| .045 in, 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr. |