OK Autrod 316L

OK Autrod 316L is a low carbon, stainless wire for submerged arc welding of corrosion-resistant steels, such as steels of the AISI 316 and 316L. Can be used in combination with OK Flux 10.93 or 10.94.

Features

OK Autrod (316L) is an extra-low carbon, stainless wire for submerged arc welding of corrosion-resistant steels of the 18Cr12Ni3Mo type, such as steels of the AISI 316 and 316L types or somewhat lower-alloyed types. OK Autrod can be used in combination with OK Flux 10.92 or OK Flux 10.93.

* This item is subject to Industry Alloy Surcharges

OK Autrod 316L
  • Welding Process
  • GMAW (MIG)

Classifications

Properties

Typical Properties
Typical Wire Analysis  
C 0.02 %
Mn 1.8 %
Si 0.4 %
Cr 19.0 %
Ni 12.0 %
Mo 2.7 %

Part No.

Autrod 316L
Part No. Model / Product Description UPC
163032311A ES OK ER316L 1/8X55#CL 000000000000
163040311A ES OK ER316L 5/32X55#CL 000000000000
163024311A ES OK ER316L 3/32X55#CL 662303077655

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr.
.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
.062 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed DCEP (Electrode Positive) Volts Deposition Rate
.030 in, 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.