Arcaloy ER316LSi is a low carbon, high silicon grade of 316. The addition of silicon improves the weldability and performance.
Arcaloy ER316LSi is a solid wire and is for welding stainless steel Types 316 and 316L and in some cases 304 and 304L. The additional silicon content over Arcaloy ER316L gives greater weld metal fluidity improves the bead shape. Depending upon its form, Arcaloy ER316LSi can be used in the MIG & TIG processes. In the case of the MIG (GMAW), spray, pulse or short-arc modes of transfer are used depending on the gas used. With this process, shielding gases of argon with 1 or 2% oxygen are commonly used for 'spray' and a mixture of 90% helium - 7.5% argon - 2.5% carbon dioxide is used for 'short-arc'. For TIG (GTAW), 100% argon or argon with some helium additions are used.
* This item is subject to Industry Alloy Surcharges

| C | 0.02 % |
|---|---|
| Mn | 1.7 % |
| Si | 0.8 % |
| Cr | 18.5 % |
| Ni | 12 % |
| Mo | 2.5 % |
| Cu | 0.15 % |
| Ferrite | 8 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 258123165 | AB ER316LSI 035X500#OMP | 662303667764 |
| 258171115 | AB ER316LSI 1/16X33#PSP | 662303027889 |
| 258173020 | AB ER316LSI 030X10#PSP/60CT | 662303027841 |
| 258173517 | AB ER316LSI 035X33#BAWS | 662303026455 |
| 258174515 | AB ER316LSI 045X33#BAWS | 662303026370 |
| 258175520 | AB ER316LSI 035X10#PSP/60CT | 662303027858 |
| 258175553 | AB ER316LSI 035X250#OMP 2/PLT | 662303667863 |
| 258175678 | AB ER316LSI 045X500#OMP | 662303667771 |
| 258176106 | AB ER316LSI 030X33#PSP | 662303027872 |
| Diameter | Wire Feed Speed | AMPS | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg/hr |
| .035 in., 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg/hr |
| .045 in., 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg/hr |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in., 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in., 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in., 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |