Arcaloy ER320LR Tigrod is designed for welding Carpenter 20Cb-3® type stainless steels.
The low residual content compared to ER320 gives increased crack resistance. The interpass temperature and stresses should be kept low. Arcaloy ER320LR is only available in GTAW rod form where the shielding gas used is 100% argon or argon with some helium additions.
* This item is subject to Industry Alloy Surcharges

| GTAW using 100% Argon | |
|---|---|
| Yield Stress | 57 ksi, 400 MPa |
| Tensile Strength | 81 ksi, 560 MPa |
| Elongation in 2" | 37 % |
| Typical Chemical Analysis | |
| C | 0.007 % |
| Mn | 1.8 % |
| Si | 0.05 % |
| Cr | 20 % |
| Ni | 33 % |
| Mo | 2.4 % |
| Cu | 3.4 % |
| Nb | 0.25 % |
| Ferrite | 0 FN |