Spoolarc 65 is a triple deoxidize (Aluminum, Titanium, Zirconium) GMAW/GTAW welding wire. It's sluggish puddle makes it suitable for out of position welding. Spoolarc 65 produces extremely good impact properties using the GTAW process.
Spoolarc 65 is a triple deoxidized (Aluminum, Titanium, Zirconium) welding wire designed for welding over rust and mill scale. The less fluid weld puddle of Spoolarc 65 makes it easy to control when used out of position. Spoolarc 65 is the preferred wire for all position welding of small diameter pipe. It is available in forms suitable for MIG and TIG welding.

| As Welded GMAW 98% Ar / 2% O2 | |
|---|---|
| Yield Strength | 70 ksi, 480 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation in 2" | 26 % |
| As Welded GMAW CO2 | |
| Yield Strength | 67 ksi, 460 MPa |
| Tensile Strength | 79 ksi, 545 MPa |
| Elongation in 2" | 26 % |
| As Welded GTAW Argon | |
| Yield Strength | 73 ksi, 505 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation in 2" | 31 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -20°F (-29°C) | |
| As Welded GMAW 98% Ar / 2% O2 | 45 ft.-lbs., 61 J |
| As Welded GMAW CO2 | 35 ft.-lbs., 47 J |
| As Welded GTAW Argon | 170 ft.-lbs., 230 J |
| Typical Undiluted Weld Metal Analysis | |
| GMAW CO2 | |
| C | 0.08 % |
| Mn | 0.9 % |
| Si | 0.3 % |
| P | 0.008 % |
| S | 0.007 % |
| GTAW Argon | |
| C | 0.06 % |
| Mn | 1.0 % |
| Si | 0.5 % |
| P | 0.008 % |
| S | 0.007 % |
| Typical Wire Analysis | |
| C | 0.04 % |
| Mn | 1.1 % |
| Si | 0.5 % |
| P | 0.006 % |
| S | 0.009 % |
| Al | 0.09 % |
| Ti | 0.08 % |
| Zr | 0.04 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 1047F10 | 65 3/32X36X30#CT F1 | 662303500696 |
| 1047F12 | 65 1/8X36X40#CT F1 | 662303500702 |
| 1041F08 | 65 1/16X36X50#CT | 662303500245 |
| 1041F10 | 65 3/32X36X50#CT | 662303500252 |
| 1041F12 | 65 1/8X36X50#CT | 662303500269 |
| 1042F04 | 65 030X44#SP | 662303500337 |
| 1042F05 | 65 035X44#SP | 662303500344 |
| 1042F07 | 65 045X44#SP | 662303500351 |
| 1042F08 | 65 1/16X44#SP | 662303500368 |
| 1044F28 | 65 1/16X65#CL | 662303500481 |
| 1047F08 | 65 1/16X36X25#CT F1 | 662303500689 |
| 1047F28 | 65 1/16X36X15#CT F2 | 662303500740 |
| 1047F30 | 65 3/32X36X20#CT F2 | 662303500757 |
| 1047F32 | 65 1/8X36X30#CT F2 | 662303500764 |
| 1048F05 | 65 035X33#SP | 662303500863 |
| 104EFDD | 65 045X35#SP E23765/1C | 662303501198 |
| 104TF44 | 65 030X11#SPX44#CT | 662303520809 |
| 104TF45 | 65 035X11#SPX44#CT | 662303520786 |
| 104UF65 | 65 035X550#OMP 20 2/PLT | 662303668143 |
| 104UF67 | 65 045X550#OMP 20 2/PLT | 662303668150 |
| 104YF30 | 65 3/32X36X10#T/60#CT F2 AWS | 662303523381 |
| 104YF32 | 65 1/8X36X10#T/60#CT F2 AWS | 662303523398 |
| 1047F34 | 65 5/32X36X30#CT F2 AWS | 662303669393 |
| 104YF28 | 65 1/16X36X5#T/30#CT F2 AWS | 662303523374 |
| 1045F53 | 65 7/32XROD COIL | 000000000000 |
| 104UF48 | 65 1/16X900#OMP 2/PLT | 662303084332 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate |
|---|---|---|---|---|
| .023 in, 0.6 mm | 100 | 23 | 400 ipm, 1016 cm/min | N/A, 2.7 lbs/hr, 1.2 kg/hr |
| 106 | 23 | 450 ipm, 1143 cm/min | 3.1 lbs/hr, 1.4 kg/hr | |
| 111 | 24 | 500 ipm, 1270 cm/min | 3.4 lbs/hr, 1.6 kg/hr | |
| 117 | 24 | 550 ipm, 1397 cm/min | 3.8 lbs/hr, 1.7 kg/hr | |
| 122 | 25 | 600 ipm, 1524 cm/min | 4.1 lbs/hr, 1.9 kg/hr | |
| 125 | 25 | 630 ipm, 1600 cm/min | 4.3 lbs/hr, 2 kg/hr | |
| .030 in, 0.8 mm | 160 | 24 | 500 ipm, 1270 cm/min | 5.8 lbs/hr, 2.6 kg/hr |
| 173 | 25 | 550 ipm, 1397 cm/min | 6.4 lbs/hr, 2.9 kg/hr | |
| 187 | 25 | 600 ipm, 1524 cm/min | 7 lbs/hr, 3.2 kg/hr | |
| 200 | 26 | 650 ipm, 1651 cm/min | 7.6 lbs/hr, 3.4 kg/hr | |
| .035 in, 0.9 mm | 180 | 25 | 400 ipm, 1016 cm/min | 6.3 lbs/hr, 2.9 kg/hr |
| 197 | 26 | 450 ipm, 1143 cm/min | 7.1 lbs/hr, 3.2 kg/hr | |
| 213 | 26 | 500 ipm, 1270 cm/min | 7.9 lbs/hr, 3.6 kg/hr | |
| 230 | 27 | 550 ipm, 1397 cm/min | 8.7 lbs/hr, 4 kg/hr | |
| .045 in, 1.2 mm | 260 | 25 | 300 ipm, 762 cm/min | 7.9 lbs/hr, 3.6 kg/hr |
| 280 | 26 | 350 ipm, 889 cm/min | 9.2 lbs/hr, 4.2 kg/hr | |
| 300 | 28 | 400 ipm, 1016 cm/min | 10.5 lbs/hr, 4.8 kg/hr | |
| 320 | 29 | 450 ipm, 1143 cm/min | 11.8 lbs/hr, 5.4 kg/hr | |
| 340 | 30 | 500 ipm, 1270 cm/min | 13.1 lbs/hr, 6 kg/hr | |
| .052 in, 1.3 mm | 275 | 26 | 265 ipm, 673 cm/min | 9.3 lbs/hr, 4.2 kg/hr |
| 310 | 28 | 300 ipm, 762 cm/min | 10.5 lbs/hr, 4.8 kg/hr | |
| 360 | 31 | 350 ipm, 889 cm/min | 12.2 lbs/hr, 5.6 kg/hr | |
| 400 | 33 | 390 ipm, 991 cm/min | 13.6 lbs/hr, 6.2 kg/hr | |
| .062 in, 1.6 mm | 290 | 26 | 180 ipm, 457 cm/min | 9.1 lbs/hr, 4.1 kg/hr |
| 310 | 28 | 200 ipm, 508 cm/min | 10.1 lbs/hr, 4.6 kg/hr | |
| 340 | 31 | 230 ipm, 584 cm/min | 11.6 lbs/hr, 5.3 kg/hr | |
| 370 | 34 | 260 ipm, 660 cm/min | 13.2 lbs/hr, 6 kg/hr | |
| 390 | 36 | 280 ipm, 711 cm/min | 14.2 lbs/hr, 6.4 kg/hr |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate |
|---|---|---|---|---|
| .023 in, 0.6 mm | 45 | 14 | 150 ipm, 381 cm/min | N/A, 1 lbs/hr, 0.4 kg/hr |
| 55 | 14 | 200 ipm, 508 cm/min | 1.3 lbs/hr, 0.6 kg/hr | |
| 65 | 15 | 250 ipm, 635 cm/min | 1.6 lbs/hr, 0.7 kg/hr | |
| 74 | 15 | 300 ipm, 762 cm/min | 2 lbs/hr, 0.9 kg/hr | |
| 84 | 16 | 350 ipm, 889 cm/min | 2.3 lbs/hr, 1 kg/hr | |
| 90 | 16 | 380 ipm, 965 cm/min | 2.5 lbs/hr, 1.1 kg/hr | |
| .030 in, 0.8 mm | 60 | 14 | 150 ipm, 381 cm/min | 1.7 lbs/hr, 0.8 kg/hr |
| 80 | 15 | 200 ipm, 508 cm/min | 2.2 lbs/hr, 1 kg/hr | |
| 100 | 15 | 250 ipm, 635 cm/min | 2.8 lbs/hr, 1.3 kg/hr | |
| 120 | 16 | 300 ipm, 762 cm/min | 3.3 lbs/hr, 1.5 kg/hr | |
| 140 | 16 | 350 ipm, 889 cm/min | 3.9 lbs/hr, 1.8 kg/hr | |
| 144 | 16 | 360 ipm, 914 cm/min | 4 lbs/hr, 1.8 kg/hr | |
| .035 in, 0.9 mm | 90 | 15 | 180 ipm, 457 cm/min | 2.7 lbs/hr, 1.2 kg/hr |
| 113 | 16 | 220 ipm, 559 cm/min | 3.3 lbs/hr, 1.5 kg/hr | |
| 137 | 18 | 260 ipm, 660 cm/min | 4 lbs/hr, 1.8 kg/hr | |
| 160 | 19 | 300 ipm, 762 cm/min | 4.6 lbs/hr, 2.1 kg/hr | |
| .045 in, 1.2 mm | 130 | 17 | 125 ipm, 318 cm/min | 3.1 lbs/hr, 1.4 kg/hr |
| 163 | 18 | 160 ipm, 406 cm/min | 4 lbs/hr, 1.8 kg/hr | |
| 200 | 19 | 200 ipm, 508 cm/min | 5 lbs/hr, 2.3 kg/hr | |
| .052 in, 1.3 mm | 150 | 17 | 135 ipm, 343 cm/min | 4.5 lbs/hr, 2.1 kg/hr |
| 173 | 18 | 160 ipm, 406 cm/min | 5.4 lbs/hr, 2.4 kg/hr | |
| 200 | 20 | 190 ipm, 483 cm/min | 6.4 lbs/hr, 2.9 kg/hr |