SPOOLARC 65

Spoolarc 65 is a triple deoxidize (Aluminum, Titanium, Zirconium) GMAW/GTAW welding wire. It's sluggish puddle makes it suitable for out of position welding. Spoolarc 65 produces extremely good impact properties using the GTAW process.

Features

Spoolarc 65 is a triple deoxidized (Aluminum, Titanium, Zirconium) welding wire designed for welding over rust and mill scale. The less fluid weld puddle of Spoolarc 65 makes it easy to control when used out of position. Spoolarc 65 is the preferred wire for all position welding of small diameter pipe. It is available in forms suitable for MIG and TIG welding.

Spoolarc 65
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • Certified By CWB TO CSA W48 ER49S-2

Properties

Typical Properties
As Welded GMAW 98% Ar / 2% O2  
Yield Strength 70 ksi, 480 MPa
Tensile Strength 82 ksi, 565 MPa
Elongation in 2" 26 %
As Welded GMAW CO2  
Yield Strength 67 ksi, 460 MPa
Tensile Strength 79 ksi, 545 MPa
Elongation in 2" 26 %
As Welded GTAW Argon  
Yield Strength 73 ksi, 505 MPa
Tensile Strength 82 ksi, 565 MPa
Elongation in 2" 31 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW 98% Ar / 2% O2 45 ft.-lbs., 61 J
As Welded GMAW CO2 35 ft.-lbs., 47 J
As Welded GTAW Argon 170 ft.-lbs., 230 J
Typical Undiluted Weld Metal Analysis  
GMAW CO2  
C 0.08 %
Mn 0.9 %
Si 0.3 %
P 0.008 %
S 0.007 %
GTAW Argon  
C 0.06 %
Mn 1.0 %
Si 0.5 %
P 0.008 %
S 0.007 %
Typical Wire Analysis  
C 0.04 %
Mn 1.1 %
Si 0.5 %
P 0.006 %
S 0.009 %
Al 0.09 %
Ti 0.08 %
Zr 0.04 %

Part No.

65
Part No. Model / Product Description UPC
1047F10 65 3/32X36X30#CT F1 662303500696
1047F12 65 1/8X36X40#CT F1 662303500702
104YF10 65 3/32X36X10#T/60#CT F1 AWS 662303523350
1041F08 65 1/16X36X50#CT 662303500245
1041F10 65 3/32X36X50#CT 662303500252
1041F12 65 1/8X36X50#CT 662303500269
1042F04 65 030X44#SP 662303500337
1042F05 65 035X44#SP 662303500344
1042F07 65 045X44#SP 662303500351
1042F08 65 1/16X44#SP 662303500368
1042F84 65 030X2#SP RANDOM WOUND 662303500429
1042F85 65 035X2#SP RANDOM WOUND 662303500436
1044F25 65 035X65#CL 662303500467
1044F27 65 045X65#CL 662303500474
1044F28 65 1/16X65#CL 662303500481
1047F08 65 1/16X36X25#CT F1 662303500689
1047F08BI 65 1/16X36X25#CT F1 BATH 662303523237
1047F10BI 65 3/32X36X30#CT F1 BATH 662303523251
1047F28 65 1/16X36X15#CT F2 662303500740
1047F30 65 3/32X36X20#CT F2 662303500757
1047F32 65 1/8X36X30#CT F2 662303500764
1048F05 65 035X33#SP 662303500863
1048F24 65 030X12#SPX48#CT 662303500894
1048F85 65 035X250#RL 662303500993
104EFBD 65 035X35#SP MIL 662303501167
104EFDD 65 045X35#SP E23765/1C 662303501198
104TF44 65 030X11#SPX44#CT 662303520809
104TF45 65 035X11#SPX44#CT 662303520786
104UF65 65 035X550#OMP 20 2/PLT 662303668143
104UF67 65 045X550#OMP 20 2/PLT 662303668150
104UF85 65 035X550#OMP 20 4/PLT 662303668402
104YF30 65 3/32X36X10#T/60#CT F2 AWS 662303523381
104YF32 65 1/8X36X10#T/60#CT F2 AWS 662303523398
1045F53 65 7/32XROD COIL 000000000000

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.

Extra Info