SPOOLARC 82

Spoolarc 82 is a premium quality wire suitable for many general purpose carbon steel MIG welding applications. Spoolarc 82 is suitable for use over light rust.

Features

Spoolarc 82 is a premium quality, general purpose MIG wire subjected to stringent quality control procedures required for certification to Military, Lloyds, and ABS specifications. Spoolarc 82 is recommended for pressure vessel and pipe fabrication, HVAC duct work, and general carbon steel structural welding.

Spoolarc 82
  • Industry
  • Mobile Machinery
  • Pipeline
  • General Fabrication
  • Automotive
  • Welding Process
  • GMAW (MIG)
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • Certified by CWB to CSA W48
    • AWS/ASME SFA5.18; ER70S-3
    • CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3)
    • ABS/AWS A5.18; ER70S-3 H4
    • MIL-E-23765/1; MIL-70S-3

Properties

Typical Properties
As Welded 98% Ar / 2% O2 Shielding Gas  
Yield Strength 62 ksi, 425 MPa
Tensile Strength 76 ksi, 525 MPa
Elongation in 2" 28 %
As Welded CO2 Shielding Gas  
Yield Strength 60 ksi, 415 MPa
Tensile Strength 73 ksi, 505 MPa
Elongation in 2" 28 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded CO2 Shielding Gas 75 ft.-lbs., 102 J
As Welded 98% Ar / 2% O2 Shielding Gas 83 ft.-lbs., 112 J
Typical Undiluted Weld Metal Analysis  
As Welded CO2 Shielding Gas  
C 0.07 %
Mn 0.9 %
Si 0.4 %
P 0.006 %
S 0.008 %
98% Ar / O2 Shielding Gas  
C 0.8 %
Mn 1.0 %
Si 0.5 %
P 0.006 %
S 0.008 %
Typical Wire Analysis  
C 0.09 %
Mn 1.2 %
Si 0.5 %
P 0.007 %
S 0.005 %
Cu 0.07 %

Part No.

82
Part No. Model / Product Description UPC
121EFABBI 82 030X12#SP/48# MIL BATH 662303523206
121EFBDBI 82 035X35#SP MIL BATH 662303523213
121EFBSBI 82 035X11#SP/44#CT MIL BATH 662303523558
121EFDDBI 82 045X35#SP MIL BATH 662303523541
1527L10 82 3/32X36X30#CT F1 EX 70S-2 662303516062
11J9C07 82 045 600#MP 4/PLT UAW AF 662303517281
11J9F41 82 052X900#MP PB PLT CFA 662303518585
11J9F47 82 045X900#MP PB PLT CFA 662303515928
1212F04 82 030X44#SP 662303504243
1212F05 82 035X44#SP 662303504250
1212F07 82 045X44#SP 662303504274
1212F84 82 030X2#SP RANDOM WOUND 662303504335
1212F85 82 035X2#SP RANDOM WOUND 662303504342
1212F87 82 045X2#SP RANDOM WOUND 662303504359
1214F25 82 035X65#CL 662303504373
1214F27 82 045X65#CL 662303504397
1217F08 82 1/16X36X25#CT F1 662303504595
1217F10 82 3/32X36X30#CT F1 662303504601
1217F12 82 1/8X36X40#CT F1 662303504618
1218F04 82 030X33#SPL 662303504656
1218F05 82 035X33#SP 662303504663
1218F24 82 030X12#SP 662303504694
1218F27 82 045X12#SP 662303504717
1218F45 82 035X60#SP 662303504731
1218F47 82 045X60#SP 662303504748
1219F05 82 035X500#MP 662303504854
1219F45 82 035X900#MP PB PLT 662303516123
1219F47 82 045X900#MP PB PLT 662303517953
121DF08 82 1/16X36X25#CT F1 662303504908
121DF10 82 3/32X36X30#CT F1 MIL 662303504915
121DF30 82 3/32X36X20#CT F2 MIL 662303522735
121DF32 82 1/8X36X30#CT F2 MIL 662303519377
121DF48 82 1/16X18 F1 MIL 662303667962
121DF50 82 3/32X18X25#CT F1 MIL 662303504939
121DF68 82 1/16X12 F1 662303504946
121EFAB 82 030X11#SPX44#CT MIL 662303504960
121EFBC 82 035X25#SP 23765/1E 662303505004
121EFBD 82 035X35#SP 23765/1E 662303505011
121EFBS 82 035X11#SP/44#CT MIL 662303520960
121EFDB 82 045X11#SPX44#CT MIL 662303505028
121EFDD 82 045X35#SP MIL 662303505042
121EFDS 82 045X11#SP/44#CT MIL 662303522179
121TF44 82 030X11#SP/44#CT 662303520762
121TF45 82 035X11#SPX44#CT 662303520687
121TF47 82 045X11#SPX44#CT 662303520694
121UF65 82 035X550#OMP 20 2/PLT 662303668167
121UF67 82 045X550#OMP 20 2/PLT 662303668174
121UF85 82 035X550#OMP 20 4/PLT 662303668617
121UF87 82 045X550#OMP 20 4/PLT 662303667870
152HL10 82 3/32X36X20#CT F1 EX 70S-2 662303522896
1218F41 82 052X60#SP 662303504724
121EFDSBI 82 045X11#SP/44# MIL BATH 662303523190
121UF21 82 052X1050#OMP 2/PLT 662303668921
121UF27 82 045X1050#OMP 2/PLT 662303668938
121UF45 82 035X900#OMP 2/PLT 662303668914

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 202 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.