Print this page

SPOOLARC 87HP

Spoolarc 87 HP features an optimized manganese to silicon ratio. It is suitable for welding over moderate amounts of rust and scale.

Features

Spoolarc 87 HP is a high manganese carbon steel wire. It features an optimized manganese to silicon ratio to produce excellent appearing welds over a wide range of welding parameters. It also produces excellent weld metal mechanical properties. Spoolarc 87 HP is suitable for welding over moderate amounts of rust and scale. This wire is widely used for robotic welding applications in the automotive industry, and fabrication of heavy equipment and farm implements. Spoolarc 87 HP is also available as a TIG rod.

Spoolarc 87HP
  • Industry
  • Shipbuilding
  • Mobile Machinery
  • General Fabrication
  • Automotive
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • CERTIFIED BY CWB TO CSA W48 ER49S-7
    • AWS/ASME SFA 5.18; ER70S-7

Properties

Typical Properties
As Welded GMAW CO2  
Yield Strength 68 ksi, 470 MPa
Tensile Strength 82 ksi, 565 MPa
Elongation in 2" 27 %
As Welded GMAW 75% Ar / 25% CO2  
Yield Strength 70 ksi, 480 MPa
Tensile Strength 82 ksi, 565 MPa
Elongation in 2" 29 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW CO2 55 ft.-lbs., 75 J
As Welded GMAW 75% Ar / 25% CO2 62 ft.-lbs., 84 J
Typical Undiluted Weld Metal Analysis  
GMAW CO2  
C 0.09 %
Mn 1.2 %
Si 0.4 %
P 0.008 %
S 0.010 %
GMAW 75% Ar / 25% CO2  
C 0.09 %
Mn 1.4 %
Si 0.5 %
P 0.008 %
S 0.010 %
Typical Wire Analysis  
C 0.08 %
Mn 0.6 %
Si 0.6 %
P 0.009 %
S 0.008 %

Part No.

87HP
Part No. Model / Product Description UPC
11FTF45 87HP 035X10LB 12 SP 662303515225
1451F08 87HP 1/16X36X50#CT F0 662303508838
1451F10 87HP 3/32X36X50#CT F0 662303508845
1451F12 87HP 1/8X36X50#CT F0 662303508852
1451F14 87HP 5/32X36X50#CT F0 662303508869
1452F04 87HP 030X44#SP 662303508883
1452F05 87HP 035X44#SP 662303508890
1452F07 87HP 045X44#SP 662303508906
1455F65 87HP 035X1000#WFRL 80-100 5 A 662303520137
1457F08 87HP 1/16X36X25#CT F1 662303509019
1457F10 87HP 3/32X36X30#CT F1 662303509026
1457F12 87HP 1/8X36X40#CT F1 662303509033
1458F05 87HP 035X33#SP 662303513771
1458F24 87HP 030X12#SPX48#CT 662303509088
1458F45 87HP 035X60#SP 662303509118
1459F05 87HP 035X500#MP 662303509200
1459F07 87HP 045X600#MP 662303509217
1459F47 87HP 045X900#MP PBPLT 662303514143
1459F48 87HP 1/16X900#MP PBPLT 662303516673
145UF47 87HP 045X900#OMP 2/PLT 000000000000
145UF45 87HP 035X900#OMP 2/PLT 662303667818
145UF48 87HP 1/16X900#OMP 2/PLT 662303668891
145UF85 87HP 035X550#OMP 20 4/PLT 662303668853
145UF87 87HP 045X550#OMP 20 4/PLT 662303668822
145XF47 87HP 045X900#OMP PBPLT 662303079840

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.