Spoolarc Easy Grind is a fully deoxidized wire designed to weld over the moderate levels of rust and paint commonly encountered in auto body repair work.
Spoolarc Easy Grind is a fully deoxidized wire designed to weld over moderate levels of rust and paint as are commonly encountered in auto body repair work. Easy Grind produces welds that easily exceed the tensile requirements of ER70S class wires.
Easy Grind is produced in small diameters and are appropriate for the low current welding machines commonly used in body shops.

| As Welded GMAW 75% Ar / 25% CO2 | |
|---|---|
| Yield Strength | 72 ksi, 495 MPa |
| Tensile Strength | 80 ksi, 550 MPa |
| Elongation in 2" | 24 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -20°F (-29°C) | |
| As Welded GMAW 75% Ar / 25% CO2 | 40 ft.-lbs., 54 J |
| Diameter | Electrode Unit Length/Wt | Amps | Volts | Wire Feed Speed | Optimum Amps | Optimum Volts | Optimum Wire Feed Speed |
|---|---|---|---|---|---|---|---|
| 0.023 in, 0.6 mm | 8505 in/lb, 476 m/kg | 45-90 | 14-16 | 150-380 ipm, 381-965 cm/min | 70 | 15 | 300 ipm, 762 cm/min |
| 0.030 in, 0.8 mm | 5000 in/lb, 280 m/kg | 60-140 | 14-16 | 150-350 ipm, 381-889 cm/min | 100 | 15 | 220 ipm, 559 cm/min |
| 0.035 in, 0.9 mm | 3670 in/lb, 206 m/kg | 90-160 | 15-19 | 180-300 ipm, 457-762 cm/min | 130 | 17 | 250 ipm, 635 cm/min |
| 0.045 in, 1.2 mm | 2220 in/lb, 124 m/kg | 130-200 | 17-19 | 125-200 ipm, 318-508 cm/min | 160 | 18 | 150 ipm, 381 cm/min |
| 0.052 in, 1.4 mm | 1665 in/lb, 93 m/kg | 150-200 | 17-20 | 135-190 ipm, 343-483 cm/min | 160 | 18 | 140 ipm, 356 cm/min |
| 0.062 in, 1.6 mm | 1150 in/lb, 64 m/kg | 290-400 | 26-36 | 180-280 ipm, 457-711 cm/min | 340 | 27 | 200 ipm, 508 cm/min |