Spoolarc Easy Grind

Spoolarc Easy Grind is a fully deoxidized wire designed to weld over the moderate levels of rust and paint commonly encountered in auto body repair work.

Features

Spoolarc Easy Grind is a fully deoxidized wire designed to weld over moderate levels of rust and paint as are commonly encountered in auto body repair work. Easy Grind produces welds that easily exceed the tensile requirements of ER70S class wires.
Easy Grind is produced in small diameters and are appropriate for the low current welding machines commonly used in body shops.

Easy Grind
  • Welding Process
  • GMAW (MIG)

Classifications

Properties

Typical Properties
As Welded GMAW 75% Ar / 25% CO2  
Yield Strength 72 ksi, 495 MPa
Tensile Strength 80 ksi, 550 MPa
Elongation in 2" 24 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW 75% Ar / 25% CO2 40 ft.-lbs., 54 J

Part No.

Easy Grind
Part No. Model / Product Description UPC
1302F83 EASY GRIND 025X2#SP RANDOM 662303506469
1302F84 EASY GRIND 030X2#SP RANDOM 662303668051
130TF43 EASY GRIND 025X11#SPX44#CT 662303520656
130TF44 EASY GRIND 030X11#SPX44#CT 662303520816

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.