Spoolarc 71 is a medium manganese and silicon subarc wire that has been microalloyed with titanium. It will produce a minimum 70 ksi tensile strength as welded or after 8 hours stress relief.
ESAB’s Spoolarc 71 is a medium manganese and silicon subarc wire that has been microalloyed with titanium. Used with 429, OK 10.62, and OK 10.71 fluxes Spoolarc 71 will produce weld deposits with a minimum 70,000 psi tensile strength in the as welded condition or after eight-hours of stress relief. When used with OK 10.62 weld deposits meet ASME A No. 1 chemistry requirements. Spoolarc 71 is used for welding pressure vessles and can be used for other applications requiring good mechanical properties after stress relieving.

| C | 0.10 % |
|---|---|
| Mn | 1.2 % |
| Si | 0.5 % |
| P | 0.004 % |
| S | 0.005 % |
| Ti | 0.07 % |
| Typical wire analysis | |
| C | 0.10 % |
| Mn | 1.22 % |
| Si | 0.55 % |
| P | 0.008 % |
| S | 0.005 % |
| Other | Ti 0.07 |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 13L4F28 | 71 1/16X65#CL | 662303668525 |
| 13L4F29 | 71 5/64X65#CL | 662303521806 |
| 13L4F30 | 71 3/32X65#CL | 662303520991 |
| 13L4F32 | 71 1/8X65#CL | 662303521813 |
| 13L4F34 | 71 5/32X65#CL | 662303520984 |
| 13L6F10 | 71 3/32X800#DR | 662303522995 |
| 13L6F12 | 71 1/8X800#DR | 662303522339 |
| 13L6F14 | 71 5/32X800#DR | 662303521981 |
| 13L4F35 | 71 3/16X65#CL | 662303669003 |
| 13L5F34 | 71 5/32X200#CL | 662303668839 |