Spoolarc 36 is a high manganese wire for single or multipass welding. Typical applications include seam welding on hot water tanks, valves, fittings, and heavy vessel fabrication.
High manganese wire for single or multipass welding. Produces higher strength levels than either Spoolarc 80 or 81 wires. Best mechanical properties, both as welded and stress relieved, are possible when used with a neutral fused flux. Spoolarc 36 can also be used for electroslag welding on mild steel. Applications include seam welding on hot water tanks, valves and fittings, heavy structural steel fabrication, and some short term postweld heat treatment.

| C | 0.13 % |
|---|---|
| Mn | 1.8 % |
| Si | 0.03 % |
| P | 0.009 % |
| S | 0.012 % |
| Typical wire analysis | |
| C | 0.16 % |
| Mn | 1.96 % |
| Si | 0.02 % |
| P | 0.014 % |
| S | 0.016 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 1094F29 | 36 5/64X65#CL | 662303501648 |
| 1094F30 | 36 3/32X65#CL | 662303501655 |
| 1094F32 | 36 1/8X65#CL | 662303501662 |
| 1094F34 | 36 5/32X65#CL | 662303501679 |
| 1095F37 | 36 5/16X200#CL | 662303076603 |
| 1096F10 | 36 3/32X800#DR | 662303501778 |
| 1096F14 | 36 5/32X800#DR | 662303501792 |
| 1096F15 | 36 3/16X800#DR | 662303501808 |
| 1096F54 | 36 5/32X700#DR | 662303501884 |
| 1096F55 | 36 3/16X700#DR | 662303501891 |
| 1096F56 | 36 1/4 600#DR | 662303501907 |
| 1098F88 | 36 1/16X250#RL | 662303518172 |
| 109LF48 | 36 1/16X400#SOMP 8/PLT | 662303668686 |
| Diameter | Amps | Deposition Rate | Average Deposition Efficiency |
|---|---|---|---|
| 1/16 in, 1.6 mm | 400 | 13.0 lbs./hr., 5.90 kg./hr. | 99 % |
| 500 | 17.0 lbs./hr., 7.71 kg./hr. | 99 % | |
| 5/64 in, 2.0 mm | 300 | 10.8 lbs./hr., 4.9 kg./hr. | 99 % |
| 400 | 14.5 lbs./hr., 6.58 kg./hr. | 99 % | |
| 500 | 18.2 lbs./hr., 8.26 kg./hr. | 99 % | |
| 3/32 in, 2.4 mm | 400 | 13.2 lbs./hr., 5.99 kg./hr. | 99 % |
| 500 | 17.0 lbs./hr., 7.71 kg./hr. | 99 % | |
| 600 | 22.0 lbs./hr., 9.98 kg./hr. | 99 % | |
| 1/8 in, 3.2 mm | 400 | 11.0 lbs./hr., 4.99 kg./hr. | 99 % |
| 500 | 14.5 lbs./hr., 6.58 kg./hr. | 99 % | |
| 600 | 18.0 lbs./hr., 8.16 kg./hr. | 99 % | |
| 700 | 21.2 lbs./hr., 9.62 kg./hr. | 99 % | |
| 5/32 in, 4.0 mm | 500 | 12.5 lbs./hr., 5.67 kg./hr. | 99 % |
| 600 | 16.0 lbs./hr., 7.26 kg./hr. | 99 % | |
| 700 | 19.5 lbs./hr., 8.85 kg./hr. | 99 % | |
| 800 | 23.0 lbs./hr., 10.43 kg./hr. | 99 % | |
| 900 | 26.0 lbs./hr., 11.79 kg./hr. | 99 % | |
| 3/16 in, 4.8 mm | 600 | 13.9 lbs./hr., 6.31 kg./hr. | 99 % |
| 700 | 17.5 lbs./hr., 7.94 kg./hr. | 99 % | |
| 800 | 21.0 lbs./hr., 9.53 kg./hr. | 99 % | |
| 900 | 25.0 lbs./hr., 11.34 kg./hr. | 99 % | |
| 1000 | 29.2 lbs./hr., 13.25 kg./hr. | 99 % | |
| 1100 | 34.0 lbs./hr., 15.42 kg./hr. | 99 % |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .023 in, 0.6 mm | 150 ipm, 381 cm/min | 45 | 14 | 1 lbs./hr., 0.4 kg./hr. |
| 200 ipm, 508 cm/min | 55 | 14 | 1.3 lbs./hr., 0.6 kg./hr. | |
| 250 ipm, 635 cm/min | 65 | 15 | 1.6 lbs./hr., 0.7 kg./hr. | |
| 300 ipm, 762 cm/min | 74 | 15 | 2 lbs./hr., 0.9 kg./hr. | |
| 350 ipm, 889 cm/min | 84 | 16 | 2.3 lbs./hr., 1 kg./hr. | |
| 380 ipm, 965 cm/min | 90 | 16 | 2.5 lbs./hr., 1.1 kg./hr. | |
| .030 in, 0.8 mm | 150 ipm, 381 cm/min | 60 | 14 | 1.7 lbs./hr., 0.8 kg./hr. |
| 200 ipm, 508 cm/min | 80 | 15 | 2.2 lbs./hr., 1 kg./hr. | |
| 250 ipm, 635 cm/min | 100 | 15 | 2.8 lbs./hr., 1.3 kg./hr. | |
| 300 ipm, 762 cm/min | 120 | 16 | 3.3 lbs./hr., 1.5 kg./hr. | |
| 350 ipm, 889 cm/min | 140 | 16 | 3.9 lbs./hr., 1.8 kg./hr. | |
| 360 ipm, 914 cm/min | 144 | 16 | 4 lbs./hr., 1.8 kg./hr. | |
| .035 in, 0.9 mm | 180 ipm, 457 cm/min | 90 | 15 | 2.7 lbs./hr., 1.2 kg./hr. |
| 220 ipm, 559 cm/min | 113 | 16 | 3.3 lbs./hr., 1.5 kg./hr. | |
| 260 ipm, 660 cm/min | 137 | 18 | 4 lbs./hr., 1.8 kg./hr. | |
| 300 ipm, 762 cm/min | 160 | 19 | 4.6 lbs./hr., 2.1 kg./hr. | |
| .045 in, 1.2 mm | 125 ipm, 318 cm/min | 130 | 17 | 3.1 lbs./hr., 1.4 kg./hr. |
| 160 ipm, 406 cm/min | 163 | 18 | 4 lbs./hr., 1.8 kg./hr. | |
| 200 ipm, 508 cm/min | 200 | 19 | 5 lbs./hr., 2.3 kg./hr. | |
| .052 in, 1.3 mm | 135 ipm, 343 cm/min | 150 | 17 | 4.5 lbs./hr., 2.1 kg./hr. |
| 160 ipm, 406 cm/min | 173 | 18 | 5.4 lbs./hr., 2.4 kg./hr. | |
| 190 ipm, 483 cm/min | 200 | 20 | 6.4 lbs./hr., 2.9 kg./hr. |
Usable with OK Flux 50, 60, 80, 124 and 585 fluxes.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.