SPOOLARC ENi4

Spoolarc ENi4 is a submerged arc welding wier that contains 1.74% Ni and 0.17% Mo. It is typically used for the welding of high-strength, low alloyed steels where higher strength and good notch toughness are required.

Features

Designed for single or multipass welding on high steels. Produces good low temperature toughness on a variety of base materials. Weld metal tensile strengths are in excess of 90 ksi (620 MPa) in both the as welded and stress relieved conditions. Applications include pressure vessels, offshore oil rigs, bridges, and other structural steel fabrication

SPOOLARC ENi4
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA5.23; ENi4
    • ABS/AWS A5.23; ENi4-Ni4

Properties

Typical Properties
C 0.17 %
Mn 0.73 %
Si 0.19 %
P 0.003 %
S 0.004 %
Ni 1.74 %
Mo 0.17 %

Part No.

ENi4
Part No. Model / Product Description UPC
2214F29 ENI-4 5/64X65#CL 662303510725
2214F30 ENI-4 3/32X65#CL 662303510732
2214F32 ENI-4 1/8X65#CL 662303510749
2214F34 ENI-4 5/32X65#CL 662303510756
2216F52 ENI-4 1/8 700#DR 662303510817

SAW

Accessories

Depositions/Paramaters

Extra Info

Usable with OK Flux 429, 10.71 and 10.62.