TIGROD ER90S-B3

TIGROD ER90S-B3 is an ER90S-B3 TIG rod that is used to weld 2.5% Cr - 1% Mo steels.

Features

TIGROD ER90S-B3 is a chrome-moly TIG rod used for joining 2.5% Cr - 1% Mo creep resistant steels. These copper-coated rods are primarily used to fabricate and repair power piping, pressure vessels, heat exchangers and boilers in the power generation industry.

TIGROD ER90S-B3
  • Industry
  • Power Generation
  • Petrochemical
  • Process
  • Welding Process
  • GTAW (TIG)

Classifications

  • Classifications/Approvals

    • AWS A5.28; ER90S-B3
    • ASME SFA 5.28

Properties

Typical Properties
Typical Mechanical Properties  
Stress Relieved 1 hr. @ 1375ºF (746ºC) GTAW 100% Ar  
Yield Strength 80 ksi, 555 MPa
Tensile Strength 91 ksi, 625 MPa
Elongation in 2" 19 %
Typical Wire Analysis  
GTAW 100% Ar  
C 0.08 %
Mn 0.6 %
Si 0.6 %
P 0.007 %
S 0.002 %
Cr 2.25 %
Mo 1 %

Part No.

ER90S-B3
Part No. Model / Product Description UPC
251JF48 TIG90SB3 1/16X36X10#T/30#CT E2 662303523459
251JF50 TIG90SB3 3/32X36X10#T/30#CT E2 662303523466
251JF52 TIG90SB3 1/8X36X10#T/30#CT E2 662303523473
251JF54 TIG90SB3 5/32X36X10#T/30#CT E2 662303523480