ER80S-B8 is a solid wire for TIG welding requiring creep strength. This 9% chromium - 1% Molybdenum TIG rod is used to weld 9% chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.
ER80S-B8 is a solid wire for TIG welding requiring creep strength. This 9% chromium - 1% Molybdenum TIG rod is used to weld 9% chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.

| Stress Relieved 1 hr. @ 1375ºF (746ºC) | |
|---|---|
| Yield Strength | 78 ksi, 540 MPa |
| Tensile Strength | 97 ksi, 670 MPa |
| Elongation in 2" | 23 % |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.09 % |
| Mn | 0.5 % |
| Si | 0.4 % |
| P | 0.005 % |
| S | 0.003 % |
| Cr | 8.8 % |
| Mo | 1.0 % |