TIGROD ER80S-B8

ER80S-B8 is a solid wire for TIG welding requiring creep strength. This 9% chromium - 1% Molybdenum TIG rod is used to weld 9% chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.

Features

ER80S-B8 is a solid wire for TIG welding requiring creep strength. This 9% chromium - 1% Molybdenum TIG rod is used to weld 9% chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.

Classifications

  • Classifications/Approvals

    • AWS A5.28; ER80S-B8
    • ASME SFA 5.28

Properties

Typical Properties
Stress Relieved 1 hr. @ 1375ºF (746ºC)  
Yield Strength 78 ksi, 540 MPa
Tensile Strength 97 ksi, 670 MPa
Elongation in 2" 23 %
Typical Undiluted Weld Metal Analysis  
C 0.09 %
Mn 0.5 %
Si 0.4 %
P 0.005 %
S 0.003 %
Cr 8.8 %
Mo 1.0 %

Part No.

ER80S-B8
Part No. Model / Product Description UPC
259971281 TIG80SB8 1/16X36X10#T/30#CT E2 662303082635
259971299 TIG80SB8 3/32X36X10#T/30#CT E2 662303082642
259971307 TIG80SB8 1/8X36X10#T/30#CT E2 662303082659
259971315 TIG80SB8 5/32X36X10#T/30#CT E2 662303082666

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.